Finally here is a link to the build I have been doing and the tig pics to go with.
http://www.starquestclub.com/forum/i...owtopic=100516
Mad-Dax
Printable View
Finally here is a link to the build I have been doing and the tig pics to go with.
http://www.starquestclub.com/forum/i...owtopic=100516
Mad-Dax
WOW, that is a lot of work. Very nice. Aluminum work on the radiator is nice too.
Well, good news, the welders getting paid for each day if not paid for already.
Thanks for posting the picture of the PowerTIG 200LX so other here know what product you are using. And there :D
Off to check out TX power guys, I need 6 injectors myself.
Oh the radiator was not my work.. sad to say...but everything else was. The injectors are from racetronix
http://www.racetronix.com/
It is so cold that I don't like to do anything outside so it is slow go for now.
Random stuff I did...may already seen.
A\C fittings...kinda hard fr m to do so small.
http://i156.photobucket.com/albums/t...DSC01222-1.jpg
http://i156.photobucket.com/albums/t...DSC01224-1.jpg
Another flange clocked alittle for more clearance of turbo.
http://i156.photobucket.com/albums/t...t/DSC01247.jpg
http://i156.photobucket.com/albums/t...t/DSC01249.jpg
http://i156.photobucket.com/albums/t...t/DSC01250.jpg
Yes messy..I had to beat with a hammer to "fix"
http://i156.photobucket.com/albums/t...t/DSC01226.jpg
EASY!!!
http://i156.photobucket.com/albums/t...t/DSC01231.jpg
Solid differential mounts
http://i156.photobucket.com/albums/t...g/IMAG0021.jpg
Twin Blow Off valve flanges..can't really see.
http://i156.photobucket.com/albums/t...g/IMAG0033.jpg
In the last two years of driving this car only two cars on the road has given me issues of not being able to pull on them...We stayed head to head..on the highway.
Nissan GT-R
AMG CLS 63
http://i156.photobucket.com/albums/t...ct/1stdyno.jpg