Share
Results 1 to 4 of 4

Thread: torch type questions

Hybrid View

Ram48 torch type questions 03-31-2011, 01:08 AM
DiabolicZ Those numbers represent... 03-31-2011, 04:46 AM
jakeru I would generally recommend... 03-31-2011, 05:37 AM
Jason On some of the torches you... 03-31-2011, 07:14 AM
Previous Post Previous Post   Next Post Next Post
  1. #1

    Default torch type questions

    Ok
    I am new to tig and would like to learn about the different torches available. I know air from water cooled but what is the differences between Wp,17, wp18, wp 20 and wp26 Will they all use the same Colette and other consumables?
    Will a Ck or weld craft fit the Everlast 250ex right out of the box?
    I am thinking about a smaller air cooled torch for my machine
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  2. Default

    Quote Originally Posted by Ram48 View Post
    Ok
    I am new to tig and would like to learn about the different torches available. I know air from water cooled but what is the differences between Wp,17, wp18, wp 20 and wp26 Will they all use the same Colette and other consumables?
    Will a Ck or weld craft fit the Everlast 250ex right out of the box?
    I am thinking about a smaller air cooled torch for my machine
    Those numbers represent different torches. I do not believe you can interchange components from one to the next. Or if you can I don't believe it is any number to any number, meaning it is limited.

    The Everlast torch has a gas line coming out of the welder that you have to hook up separate from the power lead. On my Lincoln welder it is all in one connection. Basically, another torch would have to be modified to work.
    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  3. #3
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I would generally recommend matching the torch's power and duty cycle rating to your machine's output capability while getting the torch with the smallest consumables, smallest handle, smallest cable diameter. If you put an aftermarket torch on your everlast machine, do plan on getting any adapters required to make it work.

    TIG torch family comparison (based on weldcraft specs)
    ---------------------------

    Cooling method
    ---------------
    WP-9, WP-17, WP-24, WP-26 = aircooled
    WP-18, WP-20 = watercooled

    Consumable size
    ---------------
    WP-9, WP-20 = "small" consumables
    WP-17, WP-18, WP-26 = "large" consumables

    Cable thickness
    ---------------
    WP-18, WP-26 = thick cable
    WP-9, WP-17, WP-20 = thin cable

    Handle size
    -----------
    WP-9, WP-17 = small handle
    WP-18, WP-26 = large handle

    Power & duty cycle ratings
    --------------------------
    WP-9 125 amps DC @ 60% (100 amps AC)
    WP-17 150 amps DC @ 60% (125 amps AC)
    WP-26 200 amps DC @ 60% (150 amps AC)
    WP-20 250 amps DC @ 100% (180 amps AC)
    WP-18 350 amps DC @ 100% (250 amps AC)


    Other nice features to look for:
    * higher temperature resisting materials (such as silicone, or higher temp plastics, instead of lower temp materials, and braized joints instead of soldered) - provide higher power and duty cycle rating
    * more thermally conducting metal up in the torch head (such as found in CK Worldwide torches) - provide higher power and duty cycle rating without much added weight or bulk (do take a little larger diameter / bulkier heat shield to the gas cup though)
    * silicone hose - more flexible, smaller diameter, higher temperature resisting
    * "stubby" consumables - can reduce the overall bulk of your TIG torch
    * torch switch - the factory everlast torch has a switch integrated into the handle. This feature is not usually standard. Its useful IME when you are welding something away from the bench.

    Note that the factory everlast torch is a WP-18 rated 250-350 amps @ 100% duty cycle when watercooled, which may be overkill for a 250EX which is rated 250 amps @ 60% duty cycle or 200 amps @ 100% duty cycle. You might consider downsizing to a smaller watercooled or aircooled torch that will still handle the power your machine can put out.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. #4

    Default

    On some of the torches you can interchange parts. The WP17 and WP26 for instance will share many parts. The main difference between the two is the body. I forget exactly were I read about all that but it was from the weld craft website some place. I ordered a WP17 with my unit from Alex so I would assume it will come ready to plug in and use. Maybe that is an option for you if you are looking for something similar.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

Similar Threads

  1. Tig torch switch type?
    By Skeeter in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 01-18-2017, 03:38 AM
  2. Model 26 Torch & General Torch Questions...
    By Ray C in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 08-26-2012, 03:47 PM
  3. Replies: 0
    Last Post: 07-09-2011, 07:01 PM
  4. Torch type to purchase accesories?
    By DiabolicZ in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 03-18-2011, 11:42 PM
  5. Argon gauge questions/ball type flow meter
    By Longlasting in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 13
    Last Post: 07-07-2010, 06:00 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •