    I just fired it up and welded with it for the first time... Did some aluminum beads...

    First aluminum in a few years. And from a Transformer to an Inverter it's a little weird.

    It'll take me some time to get a hang of everything.

    My initial thoughts:
    Arc starts seem.... Strong? Seems there is a stronger burst of gas upon pressing the pedal. Could seem that way because I'm welding in my basement and it's as quiet as a coffin.....
    The arc itself is great. No real problems. Everything works the way it should.
    Once I get back into the aluminum groove I anticipate things will get even better.

    So other than having to learn to weld aluminum again. And understand all the settings again. My ONLY gripe SO FAR.... The gas fitting on the back of the machine is a barbed fitting. And I can't change it without taking the machine apart. Which I'm not going to do.... So I can't use my old gas lines and regulator AT THE MOMENT....

    Once my welds are up to my standards I'll post some up.

    Cheers,
    Adam

  2. #2

    Default

    Increase the pre flow, and the arc will start smoother. As far as the fitting, its fairly easy to make an adapter with a pig tail hose and a argon fitting.

  3. Default

    Okay I'll increase the preflow.
    I know I can make an adapter... I guess I was just trying to say my only gripe with the machine is rather trivial.

    So far I am VERY pleased with this unit...

  4. #4
    Join Date
    Oct 2010
    Location
    Queensland, Australia
    Posts
    23

    Default

    To reduce that rush of gas at the start make sure your gas hoses are as short as possible. I used to have about 10 feet of hose between the flow meter and the welder but once I built my welding cart, I reduced the length of hose to less than 2 feet and it made a huge difference.

    Chris
    Brisbane Australia.

  5. #5
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Here is another thing you can do to reduce the rush of gas at the start...
    Tip for reducing wasted shielding gas
    (reduce the the ID of the hose)

    Anything to reduce the volume between the flowmeter's needle valve and the solenoid inside the machine will help. Another approach is to switch to a flowmeter with a lower pressure.
    Last edited by jakeru; 03-17-2011 at 02:41 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  6. #6

    Default

    great info there Jakeru, going to add that to my to-do list for when my welder arrives. I really dont want to have to redo things and having information like this from the get go really help alot . thanks.
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

Similar Threads

  1. My Thoughts on Everlast
    By morgaj1 in forum General Welding Questions
    Replies: 17
    Last Post: 06-24-2011, 05:26 PM
  2. 250ex initial months
    By notawelder in forum Customer Testimonials
    Replies: 3
    Last Post: 03-25-2011, 08:53 AM
  3. 256 Initial review
    By Tony_F in forum Customer Testimonials
    Replies: 14
    Last Post: 03-11-2011, 10:45 PM
  4. Superultra 205 initial review
    By agrrob in forum Customer Testimonials
    Replies: 6
    Last Post: 06-27-2010, 01:01 AM
  5. Thoughts on the CT520D
    By pmill607 in forum Introduce Yourself
    Replies: 0
    Last Post: 01-30-2009, 10:19 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •