    Why is pulsed MIG not recognized by the AWS as a acceptable method of transfer?? Does anyone know? Thanks
    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

  2. #2

    Default

    That would be a question for the AWS. I believe, because of the change in the arc, it actually goes between two forms of MIG welding, short circuit and spray transfer, and you are really welding with two separate processes and short circuit isn't considered good for HD construction...That's my guess. Though I don't have a copy of the actual 1.1 statement...Maybe someone here does.

  3. #3

    Default

    Pulsed mig welding is not all it is cracked up to be , lack of penetration etc. Too get a better understanding of it's flaws go to this site http://www.weldreality.com/pulsed_we...ndamentals.htm

  4. #4
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    Porosity in the weld was always our concern. So we always did the same thing when we were asked by the Miller rep if we wanted to try out a pulsed machine. JUST SAY NO.

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  5. #5

    Default

    Our new 250P's will have the possibility of turning off the pulse...for those situations where it is prohibited.

  6. #6
    Join Date
    Mar 2011
    Location
    Springfield, Illinois
    Posts
    139

    Default

    Hey thanks for the prompt replies. It seems pretty clear to me now. Oh another thing, right after I posted about the imig205p I went to school that night and I came to find a brand new miller 350p welder that the school had purchased for the students to practice on for northrop grumman's weld test funny huh?

    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

  7. #7

    Default

    It will be interesting to see how that unit does vertical up fillets in pulse mode, something miller pulse units have never been able to successfully for the last 30 years according to this site: http://www.weldreality.com/equipment_evaluation.htm

  8. #8

    Default

    I have never tried it, but I have been told the same thing. That pulsing overhead is begging for a spark shower.
    Everlast PP256
    Everlast Imig 205
    HF 90 am inverter tig
    Scopes, Scanners, Meters

  9. #9

    Default

    Pulsing in theory should offer more control in out of position...But Spray is a flat only process.

  10. #10
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    Quote Originally Posted by performance View Post
    Our new 250P's will have the possibility of turning off the pulse...for those situations where it is prohibited.
    Now if you could turn off the pulse on the machine that would be a different story all together. I would like the pulse machine for the ability to speed up my thin sheet work. In that case I would say yes

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  11. #11
    Join Date
    Mar 2011
    Location
    Springfield, Illinois
    Posts
    139

    Default

    Im starting to wonder if my school bought the welder because of its higher amperage rating and not because of its pulse capabilities. Hmmmmm
    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

  12. #12

    Default

    Oxide, its probably more of a political situation, with either the local welding supply salesman or the Miller rep being "buddies" with the instructor...Not saying anything is traded under the table or anything, but instructors have strong preferences for equipment based off their friendship with the local welding supply people's input...and what Miller wants to clear out or what Miller is giving an extra incentive on to "push".

Similar Threads

  1. Pulsed Arc Welding?
    By scootarida1 in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 12-06-2012, 01:04 PM
  2. Excellent Pulsed TIG article
    By earla in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 08-25-2012, 01:49 AM
  3. practice pieces-Pulsed Tig
    By cdale2002 in forum Other Custom Fabrications
    Replies: 10
    Last Post: 07-30-2010, 12:15 PM
  4. 250P pulsed mig
    By Metalux in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 02-22-2010, 02:55 PM
  5. Purchased 200 ACDC Pulsed
    By wallnut in forum Customer Testimonials
    Replies: 2
    Last Post: 05-01-2009, 12:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •