Why is pulsed MIG not recognized by the AWS as a acceptable method of transfer?? Does anyone know? Thanks
Why is pulsed MIG not recognized by the AWS as a acceptable method of transfer?? Does anyone know? Thanks
Completed Midwest Technical Institute 40 week welding/pipefitting school!!
Attending Lincoln Land Community College - Degree in Computer Programming
That would be a question for the AWS. I believe, because of the change in the arc, it actually goes between two forms of MIG welding, short circuit and spray transfer, and you are really welding with two separate processes and short circuit isn't considered good for HD construction...That's my guess. Though I don't have a copy of the actual 1.1 statement...Maybe someone here does.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Pulsed mig welding is not all it is cracked up to be , lack of penetration etc. Too get a better understanding of it's flaws go to this site http://www.weldreality.com/pulsed_we...ndamentals.htm
Porosity in the weld was always our concern. So we always did the same thing when we were asked by the Miller rep if we wanted to try out a pulsed machine. JUST SAY NO.
SHOP SETUP
Esab Migmaster 250
Everlast PowerPlasma 50
Miller Dynasty 200 DX TIG
CNC Express SQ Mill
CNC Lathe 1236
Plate Shear 12"
12" Slip Roll
4 Ton Notcher
4 Ton Hand Punch
52" 18 Gauge Foot Shear
48" Pan & Box Brake
Spot Welder
50" Slip Roll
English Wheel
Bead Roller
Planishing Hammer
60" Hand Brake
7" x 12" Bandsaw
Hand Tools
Shop (TOO SMALL !!!!! )
I don't owe anyone a dime, but I get paid to lay them down
Our new 250P's will have the possibility of turning off the pulse...for those situations where it is prohibited.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Hey thanks for the prompt replies. It seems pretty clear to me now. Oh another thing, right after I posted about the imig205p I went to school that night and I came to find a brand new miller 350p welder that the school had purchased for the students to practice on for northrop grumman's weld test funny huh?
![]()
Completed Midwest Technical Institute 40 week welding/pipefitting school!!
Attending Lincoln Land Community College - Degree in Computer Programming
It will be interesting to see how that unit does vertical up fillets in pulse mode, something miller pulse units have never been able to successfully for the last 30 years according to this site: http://www.weldreality.com/equipment_evaluation.htm
I have never tried it, but I have been told the same thing. That pulsing overhead is begging for a spark shower.
Everlast PP256
Everlast Imig 205
HF 90 am inverter tig
Scopes, Scanners, Meters
Pulsing in theory should offer more control in out of position...But Spray is a flat only process.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
SHOP SETUP
Esab Migmaster 250
Everlast PowerPlasma 50
Miller Dynasty 200 DX TIG
CNC Express SQ Mill
CNC Lathe 1236
Plate Shear 12"
12" Slip Roll
4 Ton Notcher
4 Ton Hand Punch
52" 18 Gauge Foot Shear
48" Pan & Box Brake
Spot Welder
50" Slip Roll
English Wheel
Bead Roller
Planishing Hammer
60" Hand Brake
7" x 12" Bandsaw
Hand Tools
Shop (TOO SMALL !!!!! )
I don't owe anyone a dime, but I get paid to lay them down
Im starting to wonder if my school bought the welder because of its higher amperage rating and not because of its pulse capabilities. Hmmmmm
Completed Midwest Technical Institute 40 week welding/pipefitting school!!
Attending Lincoln Land Community College - Degree in Computer Programming
Oxide, its probably more of a political situation, with either the local welding supply salesman or the Miller rep being "buddies" with the instructor...Not saying anything is traded under the table or anything, but instructors have strong preferences for equipment based off their friendship with the local welding supply people's input...and what Miller wants to clear out or what Miller is giving an extra incentive on to "push".
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST