    Default "Test pipe" welding

    I welded an automotive "test pipe" for a customer today. It was 2" tubing with probably about .065" wall thickness. It had clamped together slip joints, some of which were leaking exhaust gas. I just welded the slip joints together (fillet welds.)

    One piece was galvanized coated mild steel, another piece looked like aluminized coated mild steel, and the two end pieces were some kind of stainless steel (according to the customer.) Perfect case for 309L stainless filler rod.

    I was brought the assembly clamped in exact position it needed to be, so I didn't disturb the clamps or try to prep inside of the slip fit joint, but a cup brush did pretty well to prep the visible surfaces. I know there was a lot of junk (oxidation and soot) in between the slip joint that I didn't remove, but it actually TIG welded much more nicely than I was expecting.

    With the assembly welded, the clamps are unnecessary and will be removed by the customer. I used some low frequency pulsing to reduce heat input.

    Prepped:
    Attachment 1258

    Attachment 1257

    Welded:
    Attachment 1259

    Attachment 1260
    Last edited by jakeru; 03-19-2011 at 09:10 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  2. #2

    Default

    nice work jake.
    exactly the kind of thing i am planning to be doing with my pp205 when it arrives!!
    300whp FWD 94 Celica
    PowerPro 205 with a hack behind the mask!

  3. #3
    Join Date
    Mar 2011
    Location
    Springfield, Illinois
    Posts
    139

    Default

    Very nice work!!
    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

  4. #4

    Default

    Nice job!!
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

Similar Threads

  1. Everlast Super200P died. Performed "diode-ectomy". Now it's welding again!
    By jakeru in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 18
    Last Post: 01-27-2015, 09:24 PM
  2. First "real" TIG welding project coming up.
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 12-27-2012, 07:48 PM
  3. WTB 1-1/4" Pro Tools 105 Pipe Die
    By SeanMurphy265 in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 06-17-2012, 08:23 PM
  4. Nervous about my first "real" TIG welding.
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 22
    Last Post: 05-18-2012, 04:55 AM
  5. TIG Welding 2024 Aluminum ("unweldable" alloy)
    By jakeru in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 05-11-2011, 08:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •