Thread: A couple of beads from my new mig

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Mar 2011
    Location
    Apache Junction, Az
    Posts
    90

    Default A couple of beads from my new mig

    Attachment 1282
    Attachment 1283
    Attachment 1284
    Attachment 1285
    Attachment 1286

    I am still learning, but this mig makes it much easier to lay a smooth bead compared to my HH175.
    Hobart Handler 175
    Hobart Iron Man 230 with spool gun
    Thermal Dynamics Cutmaster 52
    Makita Cold Cut Saw

    Possible future addition:
    Lincoln Invertec V311
    or Miller Dynasty 350
    or ???

  2. #2
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    Looks good just a little splatter in a couple places. What was the wall thickness and which machine did you use.

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  3. #3
    Join Date
    Mar 2011
    Location
    Apache Junction, Az
    Posts
    90

    Default

    .083 wall
    .030 wire 75/25
    Hobart Iron Man 230

    Original settings Volt/Feed 4/30
    At 4, it hummed along, but the penetration was a little light At 4, there was zero splatter.
    I turned up the feed to 36, but again, the penetration was a little thin.
    I tried 5/36, but the weld was too hot and too much build up.
    I laid these at 5/32 pushing.
    What do you think?
    Hobart Handler 175
    Hobart Iron Man 230 with spool gun
    Thermal Dynamics Cutmaster 52
    Makita Cold Cut Saw

    Possible future addition:
    Lincoln Invertec V311
    or Miller Dynasty 350
    or ???

  4. #4
    Join Date
    Mar 2011
    Location
    Springfield, Illinois
    Posts
    139

    Default

    Looks quite nice!!
    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

  5. #5
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    you need to watch your tie in at the toes of you welds a couple of them had no tie in try pulling and not pushing
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

  6. #6
    Join Date
    Mar 2011
    Location
    Apache Junction, Az
    Posts
    90

    Default

    Quote Originally Posted by Wookie View Post
    you need to watch your tie in at the toes of you welds a couple of them had no tie in try pulling and not pushing
    Yeah, the toes at #4 volt tap were definitely not tied in, so I tried the #5 volt tap. I am still adjusting to the gun (larger and different than the gun on my HH175) and the whole welding process feels different with this machine. Probably different slope or inductance values. It is a "good" difference as oppose to a "bad" different feel.
    Hobart Handler 175
    Hobart Iron Man 230 with spool gun
    Thermal Dynamics Cutmaster 52
    Makita Cold Cut Saw

    Possible future addition:
    Lincoln Invertec V311
    or Miller Dynasty 350
    or ???

  7. #7
    Join Date
    Apr 2011
    Location
    Sasktachewan, Canada
    Posts
    95

    Default

    Not bad for your first start with new equipment. I would be interested in seeing your welds after you have worked with you mig for a couple months. New equipment always takes some time to adjust to.
    Attitude Determines Altitude

  8. #8

    Default

    For just starting out with new equipment it's not bad looking. Just wait until you've had some time on it, then take pictures. You'll see a difference. Of course that is part of the fun.... always learning and always improving over the last weld. Keep welding on.

Similar Threads

  1. PP50 after a couple of projects
    By wade23454 in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 06-01-2013, 12:43 PM
  2. A couple of pratice welds..
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 19
    Last Post: 06-28-2012, 11:31 PM
  3. Tried out my new PowerMaster226, couple questions
    By singlesupra in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 02-16-2012, 07:04 PM
  4. just bought a everlast wp20 couple questions!
    By revkev6 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 01-07-2012, 07:57 AM
  5. New Guy from Colorado with a couple of questions
    By MoparCar in forum Introduce Yourself
    Replies: 8
    Last Post: 05-05-2011, 03:07 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •