    I been tinkering around with nitinol wire. I havnt tried welding it yet. I want to see if I can weld wire together to make a loop. Anbody got some tips on this? Its little over half nickel and the rest titanium. Should just be a fast little spot weld together. I have a feeling my hardest part will be to clean up such thin wire to prepare for welding. To do that without greatly lowering its strength. It will be under tension when its done. Any information on this would be appreciated.

    Thanks
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  2. #2
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    Hit it with some scrotch bright and then acetone and weld away and watch your heat
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

Similar Threads

  1. My very first weld....ever.
    By CharlzO in forum Welding Projects and Pictures
    Replies: 2
    Last Post: 11-17-2014, 05:18 PM
  2. How to weld TALL weld beads on 1.6mm thick Aluminum Tube?
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 10-08-2013, 02:49 PM
  3. Penetration of weld and weld build up?
    By CGCINC in forum General Welding Questions
    Replies: 4
    Last Post: 07-03-2012, 08:06 AM
  4. I did it! I welded nitinol wire!
    By Nikola Tesla in forum Other Custom Fabrications
    Replies: 8
    Last Post: 04-05-2011, 05:16 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •