Does Everlast sell a small flex head TIG torch yet? I talked to Alex about this a few months ago and he mentioned that it was being worked on.

In order to fit a Flex head 125 amp WP9 size to my welder I had to do a bit of rigging with various bits and pieces not necessarily intended for the job.

Now that it is on there, the difference between using it and the bulky supplied fixed head 200 amp torch is night and day for control.

Of course, if I need to go over 125 amps I switch back to the wp26. It is always a relief to get the little torch back on for delicate stuff, which seems to be most of my welding.