    Hey guys, I have a question about eye protection while cutting with a plasma. I have been using my auto dark helmet while cutting with my PP 50 and the problem I have encountered is that on the lowest setting 9 I can't see what I'm doing. I have been looking into buying a set of shade 5 safety glasses from hellraiser and I kind of wanted to know what you guys are using. Like everyone else my eyesight is very important to me but as of yet I have not found a definitive answer on plasma cutting and eye protection.
    Thanks
    Tim
    Tim
    Powerplasma 50
    Miller 211 autoset
    Northern industrial dry cut
    Hobart 11 KW gen welder
    AO torch

  2. #2

    Default

    My helmet lets me manually set it to 5 when using my Cut50D. If your helmet won't let you go that low, then a set of safety glasses with 5 tint should work good.
    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  3. Default

    Quote Originally Posted by kenwhite View Post
    My helmet lets me manually set it to 5 when using my Cut50D. If your helmet won't let you go that low, then a set of safety glasses with 5 tint should work good.
    I have some sample helmets that i am seriously considering ( Mark has been evaluating the one style for the last few months ) these have the grinding function and the lower settings 5 is the shade i find best suited for using the plasma as well
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  4. #4

    Default

    So basically, the same goggles with a #5 lens, that you would use for Oxy/Acetly cutting, should be O.K. for plasma cutting? Is that correct?
    Tony
    Everlast PowerPro 256
    AC225 "Tombstone"
    HF 20 ton press
    Rotary 9000# two-post

  5. Default

    Powercat, I too felt like my auto-darkening helmet was a little too dark when cutting, but like yours, it wouldn't go below 9 either. I caught the auto-darkening red-flame helmet on sale at HF for around $45 and LOVE IT! Large viewing window and has a "cutting" setting that makes it PERFECT for my plasma use, as well as for grinder use. I can keep the same helmet in play as I bump back and forth between my cutter and welder. The setting knob is on the exterior, so just remember to bump it back up for welding. Oh, and it has a solar panel as well.

    TC
    TC
    _______________________
    Hobart Handler 187
    Everlast PowerPlasma 50
    Victor Torch Set

  6. #6

    Default

    osha "recommends" shade 8, but allows for a lighter shade if necessary.

  7. #7

    Default

    Quote Originally Posted by dirtyfarmer View Post
    So basically, the same goggles with a #5 lens, that you would use for Oxy/Acetly cutting, should be O.K. for plasma cutting? Is that correct?
    That's what I use, they look like fancy safety glasses (UV and shade 5) and you can find them all over the internet from $8 on up. The helmet idea works too, but bulky for me and the shade will not switch on by mistake due to HF or flashes as well.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Unhappy update

    Ok guys here is an update. My dad went and bought a set of what I believe to be class 3 cutting goggles today. About three cuts in and I took them off and told him to take them back. Tried to use my dark sunglasses once and took them off and put my helmet back on. I ordered a set of class 5 hellraiserand they should be here by next weekend. I'll report back then. Thanks for all the good input.
    Tim
    Powerplasma 50
    Miller 211 autoset
    Northern industrial dry cut
    Hobart 11 KW gen welder
    AO torch

  9. #9

    Default

    Hey Tim,

    I would not go less that #5 for sure. That must have been bright. Good news, the spots will go away.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  10. #10
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    I too use a #5 shade set of (Jackson Nemesis glasses $9), and found them to be the ones that I like the best. I also have tried #3 but found them to be to light. And yes I know what OSHA says but, it was too dark to see what I was cutting. Always protect your eyes and if it seems to bright then it most likely is.

    I don’t like to weld or cut while being blinded by a flash, and I don’t personally know any good blind welders.

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  11. #11

    Default

    Talking about Jackson, another option over glasses and goggles, Jackson makes a nice full face #5 shield for (about $18-20 around here).

    You can use it for grinding as well as plasma cutting. Light weight and good quality. If you tend to MIG and tack with your eyes closed (I know some of you do), having this shield on is a plus as well with the UV protection.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  12. #12
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    Quote Originally Posted by everlastsupport View Post
    Talking about Jackson, another option over glasses and goggles, Jackson makes a nice full face #5 shield for (about $18-20 around here).

    You can use it for grinding as well as plasma cutting. Light weight and good quality. If you tend to MIG and tack with your eyes closed (I know some of you do), having this shield on is a plus as well with the UV protection.
    Mike:
    The full face shield is a very good idea, and they are available at a good price. We own one and my son uses it all the time.

    And yes all welders develop some bad habits along the way. Except for me of course, I always refer to the welder’s handbook
    before I start the day, just as a refresher.

    DO AS I SAY, NOT AS I DO GRASSHOPPER

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  13. #13

    Default

    Funny Robert. Everyday huh while having breakfast I bet.. You should have it memorized by now.

    So you think you own enough tools, or just ran out of room for now? Very nice collection. Can you tell I am jealous

    A friend of mine uses a #5 face shield to MIG all the time (not recommended). He is 71, so figure to late to teach him now. I gave him one of our helmets that hangs nicely on a 330 tank.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  14. #14
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    [QUOTE=everlastsupport;7963]
    Funny Robert. Everyday huh while having breakfast I bet.. You should have it memorized by now.
    No not memorized yet, slow learner ya know.

    So you think you own enough tools, or just ran out of room for now? Very nice collection. Can you tell I am jealous
    Never enough tools, just too small a shop. But I am adding on as we speak.

    A friend of mine uses a #5 face shield to MIG all the time (not recommended). He is 71, so figure to late to teach him now. I gave him one of our helmets that hangs nicely on a 330 tank.
    Not recommended, but the helmet would be a good hood ornament for that 330. I will give it a try.

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  15. #15

    Default

    Where can I find safety glasses with a #5 lens that goes over eye glasses?
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  16. #16
    Join Date
    Feb 2011
    Location
    Mountain Home Arkansas
    Posts
    46

    Default

    Last edited by Robert s; 03-29-2011 at 05:20 AM. Reason: found more

    SHOP SETUP
    Esab Migmaster 250
    Everlast PowerPlasma 50
    Miller Dynasty 200 DX TIG
    CNC Express SQ Mill
    CNC Lathe 1236
    Plate Shear 12"
    12" Slip Roll
    4 Ton Notcher
    4 Ton Hand Punch
    52" 18 Gauge Foot Shear
    48" Pan & Box Brake
    Spot Welder
    50" Slip Roll
    English Wheel
    Bead Roller
    Planishing Hammer
    60" Hand Brake
    7" x 12" Bandsaw
    Hand Tools
    Shop (TOO SMALL !!!!! )
    I don't owe anyone a dime, but I get paid to lay them down

  17. #17

    Default

    Quick up date, used the shade 5 Jackson Hellraisers over the weekend and they were perfect. Very comfortable light weight and I even used them for a little lite grinding. I bought two pair, one for me and one for my 4 year old daughter so she could be cool hang out with dad in the garage.
    Tim
    Powerplasma 50
    Miller 211 autoset
    Northern industrial dry cut
    Hobart 11 KW gen welder
    AO torch

  18. #18
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Does a plasma cutter not produce as much UV as an arc welder? It would seem that if it does produce UV that the same full protection (skin) used for welding would still apply which to me would dictate a full helmet and skin coverings.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  19. #19

    Default

    Quote Originally Posted by Tritium View Post
    Does a plasma cutter not produce as much UV as an arc welder? It would seem that if it does produce UV that the same full protection (skin) used for welding would still apply which to me would dictate a full helmet and skin coverings.

    Thurmond
    It is less, but full protection is always better (and recommended). I do use glasses or Jackson full face shield back and forth, but the more you have one the better of course, gloves, sleeves, etc..
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  20. #20

    Default

    UVR is made up of several combinations of radiation,UVA, UVB, and, UVC. UVB which makes up less than 2% of UVR is the bad boy responsible for most skin cancers, and that nasty sunburn you got when you passed out in your lawn chair after a 12 pack. Nearly all sun screen protects against UVB. I personally use sunscreen every day and when I am welding or plasma cutting I use an spf 60 especially on my face. If I was a full time welder I would use a full hood but for as much as I use the plasma cutter I run more of a risk of getting skin cancer being out mowing my lawn than I do welding or cutting.
    Tim
    Powerplasma 50
    Miller 211 autoset
    Northern industrial dry cut
    Hobart 11 KW gen welder
    AO torch

Similar Threads

  1. Fixing a $1.00 Chinese measuring cup with $5.00 of Safety-Silv 56
    By fyidiy in forum Other Custom Fabrications
    Replies: 2
    Last Post: 03-07-2016, 04:01 PM
  2. Leaky regulator safety valve
    By McNair in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 01-09-2012, 12:04 AM
  3. safety...
    By aaxiss in forum Forum related Questions
    Replies: 14
    Last Post: 05-10-2011, 12:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •