I have now had my multi unit for just about a year. So far I have only used the tig and love it for that. I am new to stick but thought this project (home made boat float inflating 6 55gallon barrels for floatation ) would be a good one to try the stick on. Its an outside project as you can see at least for the tack up. The stick looks a bit messy as I am new to this. 1/8th wall tubing to 1/4 inch angle for most of it.

At this time I have 3 questions.

1. I am using 6013 rod, is this ok.

2. Not sure to use electrode neg or pos....switched back and forth but did not seem to make much difference.

3. If I want to go over all the welds by grinding and tig welding is that ok or is there contamination from the flux in the rod for me to tig weld. If I do try and tig it to clean things up I guess I should grind and brush?