    Hey guys. Here's some pics of a work in progress. We didnt get to finish because my welder decided to make some horrific noises, shoot sparks, and catch on fire He's planning on using a 8-10,000lb winch on a tray so he can use it in the front or rear of his truck. I think my tig welds are getting much better Ill post the rest after I get my unit back and we get it finished up.









    Last edited by Krookz; 03-30-2011 at 08:39 PM.
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

  2. #2

    Default

    what happened with the welder? make some horrific noises, shoot sparks, and catch on fire did this happen to the PP205
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  3. #3

    Default

    Nice work, that's gonna be sweet. Was it your 205?
    Big Willy in Rockford, Il. Power Pro 205, Lincoln 140 Mig, Oxy/Acetylene rig with a Cobra Torch, Full up Motorcycle shop.
    http://projectoldwing.com
    wruehl@hotmail.com
    Active Ironbutt Member.

  4. Default

    I have a front mount on one of my Avalanches [centered like yours], and TWO of them [where the snatch hooks used to be] on the ZR2 Blazer. I love it. A secondary benefit; if you hook a trailer to it and push the trailer into a parking spot or location, it can be done accurately at about 30MPH. It is a completely different thing driving a trailer into a spot instead of backing up. It is a GIANT and expensive pain in the ### to run the #0 wiring to the rear of the truck for that winch. Consider welding connectors to make life quick and easy. You'll need two males and four females....
    DO not take the shortcut of using the frame as a ground point. If you do and your solenoid goes out on the winch, you're done. If you run both ground and power, and the solenoid goes out, you just bypass the solenoid, wire directly to the winch [ a small premade jumper is nice] and switch terminals. Kind of a positive ground thing to reverse direction of the winch.

    I have a video on youtube [it's stupid, I won't give you the address] showing me pulling a Jeep and new Ford truck out of the desert with my silly little Blazer and it's winch. The funny thing; the Jeep had a winch and the forerunner that was there with us had a winch, neither wired up. BOTH people, and the entire group that had gathered, WERE TOO STUPID TO USE JUMPER CABLES TO ACTIVATE THE WINCH.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  5. #5

    Default

    It was my 205... The thing didnt burst into flames, but it was a small fire on the inside nonetheless. The noises were so loud my neighbor came outside to see what happened! Sounded like huge popping electircal arc's. Hopefully its just a fluke unit... not really thrilled about spending all my welding earnings on shipping to/from Everlast.







    Thanks for the tip's duckface, I will let my bud know since that's his truck. Mine has a integrated winch in the bumper and sportin dual batt's
    Last edited by Krookz; 03-31-2011 at 03:52 AM.
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

  6. #6

    Default

    It looks bad there, no doubt. I haven't seen a failure like that. Looks like an IGBT or two or three?

  7. #7

    Default

    Normally, if you loose an IGBT, it will take out the other which might take them all out. So things look real bad because of that. With the power they pump out, if there is a failure, there will be smoke and noise in most cases.

    I've not seen one like that as well, but Eric's guys will get you up and running.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Default

    We'll see what they say it should be there today. Thanks for speaking with me via email Mike.
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

  9. #9

    Default

    loosk like the insulation is also messed up in the bottom left of the pic - was then from the fan?
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  10. #10

    Default

    Quote Originally Posted by dgarnier View Post
    loosk like the insulation is also messed up in the bottom left of the pic - was then from the fan?
    Here's the full shot, I had not noticed that before...
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

  11. #11

    Default

    Quote Originally Posted by Krookz View Post
    We'll see what they say it should be there today. Thanks for speaking with me via email Mike.
    Krookz, No problem, yours is a bad one for sure, no one we can do on the phone like normal

    Really like the Avatar. EVO users myself.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  12. #12

    Default

    Receiver looks great. You have a LOT more patience than I do with welding. That is too much welding for me to even consider TIG, especially since the bumper cover hides ALL of your fantastic and laborious welds. Keep up the good work.

    You may want to consider adding some gussets or re-enforcement of some sort from the backside of the reciever tube to the mounting plate. Since the reciever hole centerline is about 3-3.5" above the attachment point of the mount there will be a lot of force against that weld in the rear. A 1/4" plate from the top of the mounting plate bent and lap welded to the top of the reciever tube will greatly reduce the possibility of a failure.
    Build it, wheel it, break it, fix it, and repeat!!!!!!!

    Tools:
    Everlast SuperCut 50 Plasma
    Century 200 Mig welder
    JD2 Model 32 Tube Bender

    Toys:
    1995 Ranger 2wd regular cab - 5.0HO Conversion - Street Machine
    1993 Ranger SuperCab - 466 BBF - Extreme offroad
    1985 F250 Regular Cab 4x4 - 460 BBF - Towing Beast

  13. #13

    Default

    Quote Originally Posted by everlastsupport View Post
    Krookz, No problem, yours is a bad one for sure, no one we can do on the phone like normal

    Really like the Avatar. EVO users myself.
    All I own are Android products


    Quote Originally Posted by deranged View Post
    Receiver looks great. You have a LOT more patience than I do with welding. That is too much welding for me to even consider TIG, especially since the bumper cover hides ALL of your fantastic and laborious welds. Keep up the good work.

    You may want to consider adding some gussets or re-enforcement of some sort from the backside of the reciever tube to the mounting plate. Since the reciever hole centerline is about 3-3.5" above the attachment point of the mount there will be a lot of force against that weld in the rear. A 1/4" plate from the top of the mounting plate bent and lap welded to the top of the reciever tube will greatly reduce the possibility of a failure.
    Thanks man. We do have plans to gusset, and add a brace on each side to the frame.
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

  14. #14

    Default

    Finally heard back on my 205... they cant find it!
    ˙˙˙ʎɐqǝ ɯoɹɟ pɹɐoqʎǝʞ dɐǝɥɔ pǝuɯɐp
    PP205 owner
    http://www.sgmedia.net

Similar Threads

  1. Replies: 0
    Last Post: 09-30-2012, 01:36 AM
  2. Front panel issue...
    By millermatic in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 08-28-2012, 03:07 AM
  3. 1996 Toyota Tacoma made into an off-road racer/mall crawler
    By Tacoma747 in forum Truck, Car and Bike builds
    Replies: 7
    Last Post: 06-06-2012, 01:25 AM
  4. Project #5 from Hooda- Springer front fork restore
    By hooda in forum On Road Fabrication
    Replies: 5
    Last Post: 10-23-2011, 03:07 PM
  5. Ultra205 Combo Unit - Lawnmower front end upgrade project
    By BigMacWelds in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 06-12-2009, 02:19 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •