Share
Results 1 to 5 of 5

Thread: changing settings while welding

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default changing settings while welding

    I guessing switching from AC to DC might be bad, but can you adjust the ac balance while welding? how about pulse setting? how about amps? I guess it might be easier to ask what setting shouldnt be adjusted while welding
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  2. Default

    Quote Originally Posted by dgarnier View Post
    I guessing switching from AC to DC might be bad, but can you adjust the ac balance while welding? how about pulse setting? how about amps? I guess it might be easier to ask what setting shouldnt be adjusted while welding
    Jody on weldingtipandtricks.com was adjusting the frequency while the machine was running.

    It is usually a good practice to not adjust stuff while an arc is going. I tend to play it safe and follow that practice. But, that still doesn't answer the question...
    10.3 @ 134mph 1.5 60' DA 7500ft Bandimere speedway
    http://www.youtube.com/watch?v=leUB4PCv0mU

    Lincoln PT185
    1980's Miller Plasma cutter
    Everlast LX225 here and working well.

  3. #3

    Default

    I haven't changed while welding but have changed TIG amperage, and pulse settings while the pedal/trigger was depressed (no arc) with no obvious issues...
    PowerTig 225LX
    PowerCool W300
    PowerPlasma 60S
    Miller 140 MIG

  4. #4
    Join Date
    Oct 2010
    Location
    Queensland, Australia
    Posts
    23

    Default

    You can certainly change amperage, ac frequency, and ac balance. I have a mate do it while I’m welding to see what difference it makes. I think you could change the pulse settings also.

  5. #5

    Default

    The issue with working with changing amp settings etc, are mainly with transformer machines, with switches and contacts arcing between the switch points because the current passes through them.

    While I agree, changing between polarity on our welder while welding isn't a smart idea, I honestly can't say anything would happen, mainly because I never "wanted" to find out what would it I did. But changing amps, freq. etc should be fine because they are controlling things electronically.

Similar Threads

  1. Changing to a gas lens what do I need.
    By PeterA in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 11-09-2012, 05:56 PM
  2. Project #3 from DVA: Stool for changing brakes
    By DVA in forum Other Custom Fabrications
    Replies: 7
    Last Post: 10-19-2011, 04:19 AM
  3. Changing gas to Mig Aluminum
    By Ram48 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 5
    Last Post: 08-12-2011, 02:15 AM
  4. Welding thickness amp settings
    By Mad-Dax in forum TIG Welding (GTAW/GTAW-P)