    Here are pictures of my first Tig beads with filler rod
    I am looking for input to make me better. Please let me know what you see both bad and good (if there is good it was by accident at this point)
    Everlast 250 EX
    1.5 Lanth electrode
    er70s-2 3/ 32 filler 125 amps on 4T setting
    Mild steel 1/8 plate.
    Thanks
    Ray

    Pic #1
    Attachment 1502

    Pic #2

    Attachment 1503

    Pic #3
    Attachment 1504

    Pic #4
    Attachment 1505

    Pic #5
    Attachment 1506
    Last edited by Ram48; 04-06-2011 at 09:07 PM.
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

Similar Threads

  1. My first welds with my PA 160 STH
    By ironmanjay in forum Stick Welding (SMAW)
    Replies: 9
    Last Post: 07-25-2013, 03:23 PM
  2. First TIG welds
    By 2tailfins in forum Hobyist Projects
    Replies: 9
    Last Post: 09-28-2012, 02:56 PM
  3. A few of my first welds with the I-MIG 200.....
    By CGCINC in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 26
    Last Post: 04-23-2012, 03:46 PM
  4. My Welds
    By Oxide00 in forum Other Custom Fabrications
    Replies: 35
    Last Post: 11-09-2011, 11:23 AM
  5. how are my welds
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 05-20-2011, 01:46 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •