  1. Default TIG torch consumables recommendations

    Does anyone know or have a link that gives general combination's of collet body/gas lens and cup size by a given tungsten diameter and/or amperage?
    Trying to get an order together to cover the WP9 and WP26 torches.
    Thanks in advance!

  2. #2

    Default

    Rengaw,
    The manual has a little bit of that in there in regard to amps and tungsten size. However, cup size is related to application, more than amperage.

  3. #3
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Here is a useful starting point:
    "Guide for Shield Gas Flows, Current Settings, and Cup Selection"
    http://www.ckworldwide.com/tech-3.pdf
    Last edited by jakeru; 03-11-2011 at 04:45 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  4. #4

    Default

    Hello,

    Ive been using weldcraft rare earth tungsten. Ive mostly worked on stainless with it. They have been working fine for me. Problem is I am not an expert and not absolutley sure everything that is suppose to be ideal. It doesnt seam to bead up on me or anything. The tip does round out a bit after some good current through it. Anybody who knows what they are doing used these?
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  5. #5

    Default

    Quote Originally Posted by Nikola Tesla View Post
    Hello,

    Ive been using weldcraft rare earth tungsten. Ive mostly worked on stainless with it. They have been working fine for me. Problem is I am not an expert and not absolutley sure everything that is suppose to be ideal. It doesnt seam to bead up on me or anything. The tip does round out a bit after some good current through it. Anybody who knows what they are doing used these?
    Check out http://www.weldcraft.com/pdfs/WP9ENG.pdf and http://www.weldcraft.com/pdfs/WP26ENG.pdf there is a nifty chart that show the proper parts combination.
    Lincoln Weld-Pak 100 (C-25 or CO2 Shield)
    Victor Oxy-Act
    Lincoln AC225 Tombstone
    Everlast 250EX & W300 Cooler

Similar Threads

  1. Consumables for S45 torch
    By jorgemm in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 01-12-2016, 07:48 AM
  2. PP50 consumables, ipt60 torch
    By WhitsonMetal in forum Everlast Plasma Cutters (PAC)
    Replies: 9
    Last Post: 10-08-2015, 03:55 PM
  3. Torch recommendations
    By MR2 Josh in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 06-15-2013, 03:43 PM
  4. Asking for lighter torch recommendations for the i-Tig-200
    By seanm in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 04-12-2012, 01:30 AM
  5. TIG Torch Consumables
    By bigjoeinkg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 04-27-2011, 01:37 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •