In regards to different arc voltages, I hooked my volt meter up to my stick welder and filmed the screen while i welded. I tried an 1/8 6011 and an 3/32 7018. the 6011 ran between 26 and 30 volts while the 7018 ran between 20 and 22 volts. Both were ran at the same setting of 90 amps dcep. I will try to put the video up on YouTube.