1/8th thick not sure what type of steel it is so I just used er70s2 3/32 filler
A 80amps 1/16 tungsten Seemed cold
B 80amps 3/32 tungsten Seemed cold
C 115amps 3/32 tungsten Stopped too long at the end of the weld
D 100amps 3/32 tungsten Stopped too long at the end of the weld and got a crater
E 100amps 1/16 tungsten Seemed good but I jerked in the middle and didnt keep and even bead
F 115amps 1/16 tungsten I took too long to get going and got a puddle on the back side
Front
Back
![]()