Share
Results 1 to 4 of 4

Thread: 7014 is great stuff

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default 7014 is great stuff

    Or at least forgiving for the beginner. I made some fairly pretty welds today... well, in comparison to my 6011 attempts that is. No weld pics, my self image couldn't stand the abuse.

    Here's a pic of the end product. A hiller/bedder for my garden tractor. A buddy welded up the T frame a few weeks ago with this 110v mig and I finished up the brackets and attach points with the PA200 today. --Ian

    Attachment 1815

  2. #2

    Default

    I learned how to stick weld with 7014s. They don't care about polarity and work well with AC. If you run a good bead, the slag will curl off as the weld cools. They also run pretty good at lower-than-rated amp settings.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  3. #3

    Default

    The box said 120-145 and I was running 110. I read someplace that DC was about 10 or 15% hotter than AC so I figured I was effectively at about the starting amps.

    Ian

  4. #4

    Default

    I would get good results with 90 amps dcep or dcen. My cheap HF stick welder could only muster 90 amps.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Similar Threads

  1. 50 pound box 1/8" Hobart 7014 Welding Rod
    By cbmkr in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 09-19-2013, 02:48 PM
  2. My new stuff
    By broberts5 in forum Customer Testimonials
    Replies: 4
    Last Post: 03-20-2013, 05:56 AM
  3. Replies: 1
    Last Post: 03-07-2011, 04:34 PM
  4. just got my stuff
    By Nick1969 in forum Introduce Yourself
    Replies: 1
    Last Post: 02-11-2009, 12:15 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •