First tig welding attempts, and wp26 torch questions
Hey all, got my power pro205 in Monday, and have been playing with the tig.
I've never tig welded before, only welding experience I have is messing around with my 110v mig welder welding up exhausts and what not in the garage.
A buddy gave me a peice of ~3/16" aluminum diamond plate he had laying around, so that's what I started on. These pics are the first 3hrs of practice.
Various settings thruout, but the last couple pics are setup with:
3/16" aluminum diamond plate ( welding on the backside)
3/32 2% thoriated tungsten, sharpened to a dull point
3/32 4043 filler
~120-125 amps or so
AC freq. ~1:00
AC balance ~10:00
No pulse
A hair of pre and ~ a few seconds of post flow


I was pretty happy with the bead in the middle of this pic

Suggestions and comments are welcome and needed!!!
At least I feel like the hrs spent on jodys site helped alot, definitely would suggest to anyone starting out to make the time to go thru jodys site and watch and read as much as you can, lots of helpful info and as he calls it, "no bull, no frills, down and dirty welding tips and tricks!"
For those who don't know who I'm talking about, his site is www.weldingtipsandtricks.com
Also learned alot from you guys as well!!