worntorn some higher amp stick with PU... 05-06-2011, 03:23 PM
geezer Sounds like that welder is... 05-06-2011, 08:15 PM
everlastsupport Can't see the bottom, but... 05-07-2011, 12:18 PM
Previous Post Previous Post   Next Post Next Post
  1. #1

    Default some higher amp stick with PU 205

    I've got an onsite job for the little PU205 portable multifunction. This will involve 60-80 hours of fabbing structural steel for an unusual style of home a Customer is building.
    The welding will be all stick welding and there will be some plasma cutting as well.

    I thought I would use the little Everlast instead of my Miller Onan beast. This way I don't have to spend $10 per hour just on gasoline, plus it's quiet.

    But how does it handle 1/8" 7018 on 1/4" steel?

    Have a look, so far I like it better than the Miller for this.
    This was done at 140 amps, so lots of juice left.

    Glen
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

  2. #2

    Default

    Sounds like that welder is gonna pay for itself on this one job, saving the gas money is a sure start, as usual you show a nice bead.

  3. #3

    Default

    Can't see the bottom, but don't think I need to. Looks good. Make sure you have good air flow around the unit. The PT and PP series are more commercial grade, but you should be OK.

    Using 205 and stick, you are saving gas in two ways I have people, friend of a friend, they get stick welds. Plus no worry about fans or wind.
    And like Geezer said, nothing like paying for the unit on a job right away. Good work.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Power I Mig 200 MIG STICK WELDER , how high should the amp gauge read on stick side
    By Tim L Rogers in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 01-22-2016, 04:42 AM
  2. Tig (ac/dc), mig, stick, plasma
    By scootarida1 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 11-27-2014, 01:25 AM
  3. The joy of DC stick
    By JohnT in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 08-25-2014, 01:56 AM
  4. Anybody use their 250 EX with the stick?
    By Nikola Tesla in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 03-28-2011, 01:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •