gas lenes - frist welds not so good
stopped by HTP today and picked up a gas lense kit. I tried the 3/32 body with a #8 cup..I left the flow at 12cfh,but arc wanted to wonder quite a bit, and I got a rust colored soot like coating around the weld on steel. The weld looked really bad lot of holes. I looked on line and found some places say to turn the gas up while ours say to turn it down. I was going to other setting but noticed the argon gague was down around 1300psi, so I called it a night and will get a refill in the next day or two
if your using a gas lense what flow rate do you use? what cup?
sold my miller mig
got a PT250EX
saving up for a plasma cutter