  1. Default I-Tig 200 post flow "stuck"?

    Any help is appreciated.

    As of about a month ago when I take pressure off the foot pedal sometimes the argon flow will not stop and I have to bump the pedal again to stop the flow (on the rare occasion twice). I always hear the click of the switch on the pedal when the pressure is taken off the pedal. Would I be wrong to assume it may be the solenoid sticking/not functioning properly? When it does keep flowing, if I shut off the machine the gas flow does not stop either.

  2. #2

    Default

    hook up the switch, and set the post flow to 0 and put it in 2t. Then tap the button and see if the gas stops, if not then you have a problem.
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  3. #3

    Default

    zach,
    possibly contamination in the solenoid seat or shaft. It can be cleaned out.

  4. #4
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    Quote Originally Posted by kenwhite View Post
    Mark, what do you recommend cleaning it out with? WD40?

    NO! don't use anything with oil.

    Call me, X207.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

Similar Threads

  1. Another "issue" with gas flow
    By JohnT in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 04-30-2018, 08:11 PM
  2. Everlast Super200P died. Performed "diode-ectomy". Now it's welding again!
    By jakeru in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 18
    Last Post: 01-27-2015, 09:24 PM
  3. Replies: 11
    Last Post: 10-30-2012, 06:43 PM
  4. Can't post photos, get "Internal Server Error"
    By DaveO in forum Forum related Questions
    Replies: 2
    Last Post: 03-18-2012, 02:31 PM
  5. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •