  1. #1

    Default Catch Can / Attempt at TIG welding!!

    So this is my second TIG project that I decided to do on budget with materials laying around. Never touched a TIG before my exhaust and this. It is a simple catch can for my car so I don't run the crank case vent into the intake and track oil through my intake manifolds and intake runners and then burn it. This will allow the oil to fall to the bottom of the can and the vapors to exit out of the filter. Like I said this was my second time with a TIG and any advice would be accepted.

    Filler was 1/16 308L
    1/16 1.5% Lanthanated Tungsten
    ~45 Amps
    16ga 304 stainless
    5 - 7 LPH Argon
    The nipple were made from Galvanized steel pipe and ground on a little but I don't think enough.. Still was hard to weld to.

    I started with 2 pieces of the pipe.


    Cut one in half and then flattened and then cut/ground into circles for the top and bottom lids


    Welded top and bottom on. I started using filler but it was leaving a thick bead as there was a slight edge on the top and bottom pieces that melted. These ended up being done with no filler rod used. About 1 to 2 inches at a time between rotation..





    Here you can see the nipples added on. The one on the side was pushed into the can a little and then the top sat against the surface. I think these still had some of the galvanized coating as they popped some and turned everything all white. I wire brushed them after the weld was complete.




    And installed it into the car..
    Last edited by Jason; 05-20-2011 at 08:02 AM.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  2. Default

    That project [or ones just like it] are the exact reason I bought the 256. No one wanted to do them for me, I'll have to do them myself.
    A thousand things like that I can make for the boats and the cars.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  3. #3

    Default

    The welds are nice, but oil caught in the can will vaporize and the fumes will coat the engine black, back in the old days the vent pipe went to a point at the bottm of the oil pan to be blown under the car. The workmanship is very good but I'm not too keen on the design concept. actual use will prove my point.

  4. #4

    Default

    Quote Originally Posted by geezer View Post
    The welds are nice, but oil caught in the can will vaporize and the fumes will coat the engine black, back in the old days the vent pipe went to a point at the bottm of the oil pan to be blown under the car. The workmanship is very good but I'm not too keen on the design concept. actual use will prove my point.
    Thanks.. I have been running just a filter on the vent for some time and there is no coating but the oil dripped and burned off. I was planning to run this for some time and then when I am working again I plan to design a new can that will actually have another hose at the bottom that drains back into the pan. Also when I make the next, I plan to make use of AN fittings and have it actually look nice. With our motors, we dont have any way to drain back unless we weld a bung on the oil pan. There is only the one place for it to vent and I didnt want to let the oil blow under the car as it likes to track on the back of the car then and that would suck for people behind me How bad do you think this would be for say a month or two?
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  5. #5

    Default

    Quote Originally Posted by Jason View Post
    Thanks.. I have been running just a filter on the vent for some time and there is no coating but the oil dripped and burned off. I was planning to run this for some time and then when I am working again I plan to design a new can that will actually have another hose at the bottom that drains back into the pan. Also when I make the next, I plan to make use of AN fittings and have it actually look nice. With our motors, we dont have any way to drain back unless we weld a bung on the oil pan. There is only the one place for it to vent and I didnt want to let the oil blow under the car as it likes to track on the back of the car then and that would suck for people behind me How bad do you think this would be for say a month or two?
    Dunno, all depends on the driving and condition of the motor, you should see road dust sticking to any oil on the motor, could work okay for a long time. At one time motors vented on the rocker covers and it worked until the engine started to wear then the engine got oiled. the down pipe was standard, you could always tell a worn engine by the amount of oil on the rear end of the trunk or tailgate.

  6. #6

    Default

    Quote Originally Posted by geezer View Post
    Dunno, all depends on the driving and condition of the motor, you should see road dust sticking to any oil on the motor, could work okay for a long time. At one time motors vented on the rocker covers and it worked until the engine started to wear then the engine got oiled. the down pipe was standard, you could always tell a worn engine by the amount of oil on the rear end of the trunk or tailgate.
    hmm I recenetly did a lot of work to this motor including a bump in compression and when doing so I noticed more oil loss through the vent. I wonder if it would help to have like a SS wool right below the filter. That would prevent the oil residue from coming out wouldnt it?
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  7. Default

    looks good. I just routed mine down under the truck. People always think something is wrong when ya see smoke coming from under it, but I just used 3/4" heater hose to keep the oil out of the intercooler and turbo. Mine's a powerstroke and you'd be amazed at the amount of people out there who think a diesel is right up there with a rocket motor as to how they work
    http://www.ideadevgroup.com/

Similar Threads

  1. Aluminum Tig welding - 1st attempt w/ PowerPro 205
    By inthefrey in forum General Welding Questions
    Replies: 3
    Last Post: 08-21-2013, 03:12 AM
  2. First Attempt at an Aluminum Fillet Weld
    By blasphemy000 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 08-11-2012, 10:30 PM
  3. Turbo Oil Catch Can
    By scootarida1 in forum On Road Fabrication
    Replies: 4
    Last Post: 06-26-2012, 08:55 PM
  4. My first attempt to use filler metal practice stainless steel
    By Vinhtec in forum TIG Welding (GTAW/GTAW-P)
    Replies: 17
    Last Post: 04-25-2012, 02:51 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •