    Those wire standoffs on some plasma torches (PP 50 - S45 torch ) can be a pain, they get lost, broken or what ever and they cost when you go to replace them.

    Today I decided to end that problem.

    Bought a piece of 1 inch dowel, drilled a 13/32 hole in it and sliced off a bunch of little wooden washers 0.490 thick. They fit snugly on the torch tip and they maintain the 1/8 torch height that the wire standoff did and the best part is: they act as 1/2 inch offset guide for the torch to slide along a piece of flat bar for making nice straight cuts.

    Try it you may like it, so far it is working for me.

    Come to think of it , if you want to cut circles or arc's just drill a 13/32 hole in a piece of 1/2 inch plywood and another anchor hole for a bolt and you have a cheap circle cutter for your pp 50 torch.
    Last edited by geezer; 05-24-2011 at 10:50 PM.

Similar Threads

  1. Plasma cutter wire standoff
    By ljdm1956 in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 02-21-2014, 09:25 PM
  2. PP 256 S75 Plasma torch red wire connection
    By Schuh in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 04-08-2013, 08:39 PM
  3. Supercut50P Torch Black Wire ??
    By cbmkr in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 07-12-2012, 09:02 PM
  4. plasma torch
    By shawn in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 05-14-2011, 02:07 AM
  5. Standoff for Supercut 50
    By rinktumbody in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 03-01-2010, 05:26 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •