Originally Posted by
ScratchStart
Is that an alloy wheel? or all aluminum? What kind of filler did you use?
They are good looking. I think you should CHROME them... but I am a pretty simple guy, and like shiny things...LOL
The wheel is definitely an "alloy" wheel. Pretty much nothing is made of pure aluminum as it is extremely soft and has almost no structural use at all. There are filler alloys specifically made for casting repair, but alot of people use the standard's; 4043 or 5356.
If the wheel is cast (which this one most likely is), you will likely still retain most of the strength. If it is forged or billet, the strength will go to crap if you weld it. Doesn't mean it won't work, but it will not be nearly as strong in the welded and heat affected zone.
Everlast 200DX
Everlast PT185
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile