I bought a 99 Mustang GT a while back and it came with a set of 18" Saleen wheels that had been curb rash'd nearly to death. All 4 wheels had damage. The wheels are pretty good looking and worth decent money so I decided to fix them.
I had them blasted and then tigged up the rash. Next up is to take them to work and run them through the lathe to recut the lips and then powdercoat them.
I'll throw up some updated, "fixed" pictures as soon as I can get them coated.