Now I don't have many pics of this project and it was a fast repair that allowed the car to be safe to drive. The strut tower broke on top and rusted. After some time it started to tear the metal down the back side and then continued around the side to the front. There was only a section on the front that was held together still so it was time for some repair. After cutting the tower out, it appeared that there was rust inside behind the tower at the bottom of the rain tray. The car must have had a bad sealed spot or something for it to rust from the inside out like it did. Anyways a friend had a similar car that he was going to scrap the shell from and the towers were pretty much the same as my car. The main difference between the two is the outer skins.
The car without tower
Attachment 2065
Now the tower taken from the other car was stuffed in from the bottom and put into place where the old tower existed. There was about a 1inch bead welded at the top to the inner fender and then spot welded the rest of the way across the top to the inner fender. The bottom was spot welded inside the wheel-well and there was a spot in the wheel-well that needed a patch. After the tower was in, 3M brush-able seam sealer was used any place that two pieces of metal came together and then black primer was sprayed to cover any exposed metal.
Here is the new tower in
Attachment 2063
Attachment 2064
Attachment 2066
All the surface rust was wire brushed off before the new tower was put in. This project also was done on 2 different days but at the same time as other projects. If I can find any other pictures, ill add them then.
Jason
Everlast 255EXT - Perfection
Everlast PowerPro 256 - UPS Demolished
Everlast MTS200s
12 Ton Shop Press
DeWalt Hand Tools/ChopSaw