    ......So I was welding today on AC, finished that part and switched to DC to do another and as soon as I struck the arc, (using the pedal), to tac a part, it blows through.
    When I looked at the control panel, the ampreage display read 478. The amperage control dial did not change the number indicated. I tried several other different settings and nothing worked.
    Next thing I tried was shutting it down and letting it sit for a few minutes hoping something would reset........same result.

    Does anyone have any guesses as what my problem could be?

    Thanks,

    Ken
    Last edited by Jetfire3; 06-10-2011 at 02:22 AM.
    PowerTIG 250EX
    Power Cool 300
    Hobart 210MVP

  2. #2

    Default

    Its the 4053 chip. Contact someone in support or warranty to get it seen about.

  3. #3

    Default

    I'll call tomorrow.

    Thanks Mark.
    PowerTIG 250EX
    Power Cool 300
    Hobart 210MVP

  4. Default

    damn, wish I could get that kinda amperage
    http://www.ideadevgroup.com/

  5. #5

    Default

    Yeah, it would've been great if I needed it and more importantly, was EXPECTING it!!

    Quote Originally Posted by Timberwolf View Post
    damn, wish I could get that kinda amperage
    PowerTIG 250EX
    Power Cool 300
    Hobart 210MVP

Similar Threads

  1. PowerUltra 205P stuck AMPs, not triggering solenoid neither HF start
    By Osvane in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 03-12-2018, 01:13 AM
  2. PP 256S stuck at high amperage
    By Superiorweld in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 07-08-2015, 11:27 AM
  3. Power Pro 256 stuck at 240+ AMPS
    By acannell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 19
    Last Post: 11-05-2014, 03:00 PM
  4. PowerTig 200DX Stuck in AC - help!
    By silverbullet in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 07-12-2013, 11:11 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •