inside corner joint - whats the secret
I gotten the hang of running beads and butt welds on both steel and aluminum, but the inside corner joint is not woring too well. The arc favors one side or the other, some times I get the tungsten point so close to the side the arc jumps out the side of the tungten to got to the other side. My latest attemps have been on 3/16" wall 1" square aluminum tube welding tee's. For the 2 butt welds I can run a nice bead and looks like a stack of dimes with a few nickels mixed in. I could call it good enought with just the two welds, but I would like to learn the inside corner before I get started on another project. I am using a 2% cerited 3/32 tungsten and 3/32 4043 filler #7 cup and 10 cfh
sold my miller mig
got a PT250EX
saving up for a plasma cutter