  1. #1

    Default Project #6 from Jason: Euro Radiator Support Repair.

    So I had purchased this euro rad support used from someone and it happen to be broke during shipment from UPS.. My claim with UPS was denied as they always do. I have only got one thing taken care of which they lost and to get that claim approved I had to argue and make a hassle out of it as they denied it first. Anyways since UPS was not going to do anything about it, I went to see a friend who had a plastic welder.

    Here is the broken support


    When I got to his shop, he could not find his plastic welder but that did not stop us. A soldering iron was used to V out the cracks and then a hot glue gun was used to fill it in with new plastic/rubber. It worked well as the glue melted in to penetrate the plastic.


    Since this is going to be used on my car that is getting a major custom build, I could not accept how it looked. Sanded down the glue.


    Next came some spot putty.


    and fixed waiting for paint but that will be awhile as the car is going to take awhile.


    Took a couples hours total to fix but part of that was just screwing around which is common when we hang out at the shop
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  2. #2

    Default

    I think the forum needs a new category for plastic welds.
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

Similar Threads

  1. Project #10 From Jason: Stripped Lug Bolt.
    By Jason in forum Personal Projects (no welder required)
    Replies: 10
    Last Post: 03-24-2012, 09:29 PM
  2. project 1 from Ogorir: ducting in a radiator
    By ogorir in forum On Road Fabrication
    Replies: 13
    Last Post: 10-14-2011, 06:45 PM
  3. Project 14 from Jason: Scout
    By Jason in forum Welding Repairs
    Replies: 10
    Last Post: 07-31-2011, 05:48 AM
  4. Project #5 from Jason: Exhaust #2.
    By Jason in forum On Road Fabrication
    Replies: 2
    Last Post: 06-13-2011, 05:56 AM
  5. Project 3 from Jason: Fender Roller.
    By Jason in forum Other Custom Fabrications
    Replies: 2
    Last Post: 06-02-2011, 07:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •