    Default Powder Coating Oven

    I saw some reference to powder coating in other posts so I thought I would show you mine. Maybe show some one its not that hard to do.
    Basically I shortened two 55 Gal drums and joined them as shown. Made an outside cover to hold the insulation. I used two 2300 watt stove top burners and a PID (temp controller) and a solid-state relay for the heating system. These parts are on Ebay at a good price. I made mine for horizontal use and I stand it up for storage. It has wheels and rolls like a wheel barrow. I have a trolley to hang the parts on that slides into the oven. The part shown on the trolley is a Bead Roller frame.

    Have fun
    Tom
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	oven cnstruction (5) a.jpg 
Views:	3359 
Size:	138.9 KB 
ID:	2574   Click image for larger version. 

Name:	powder coat trolly.jpg 
Views:	671 
Size:	136.9 KB 
ID:	2575   Click image for larger version. 

Name:	powder coat oven (4).jpg 
Views:	824 
Size:	138.9 KB 
ID:	2573   Click image for larger version. 

Name:	powder coat oven controller (1).jpg 
Views:	600 
Size:	139.8 KB 
ID:	2572   Click image for larger version. 

Name:	powder coat oven (7).jpg 
Views:	815 
Size:	139.8 KB 
ID:	2576  


    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  2. Default

    That's really nice looking.

  3. #3
    Join Date
    Mar 2011
    Location
    Springfield, Illinois
    Posts
    139

    Default

    Really cool, may I ask what do you plan to powder-coat??
    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

  4. #4

    Default powder coating parts

    HI Ozide00
    I do small parts for different projects, like handles and guides. The biggest things have been frames for bead rollers I have made (see attached). I did parts under the hood of my street rod that hold the hood on. On parts that may see heavy use, if done right the shine is great and holds up great.
    Basically you spray an electrically charged powder on metal parts and bake them at 350 to 425 degrees for about 10 to 15 minutes. This melts the powder and fuses it to the surface. The oven size dictates how large parts can be to powder coat.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	quick calmp and release (5).jpg 
Views:	447 
Size:	143.3 KB 
ID:	2639   Click image for larger version. 

Name:	3rd bead roller (2) A.jpg 
Views:	533 
Size:	94.1 KB 
ID:	2640   Click image for larger version. 

Name:	3rd bead roller (10) A.jpg 
Views:	499 
Size:	141.3 KB 
ID:	2641  

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  5. #5
    Join Date
    Mar 2011
    Location
    Springfield, Illinois
    Posts
    139

    Default

    Wow, now that is awsome!
    Completed Midwest Technical Institute 40 week welding/pipefitting school!!
    Attending Lincoln Land Community College - Degree in Computer Programming

Similar Threads

  1. powder coating
    By Rodsmachineshop in forum Everlast Plasma Cutters (PAC)
    Replies: 6
    Last Post: 05-18-2012, 08:38 AM
  2. two dollar rod oven
    By geezer in forum Stick Welding (SMAW)
    Replies: 20
    Last Post: 01-22-2012, 01:57 PM
  3. Powder Coating Gun Sale
    By acourtjester in forum Personal Projects (no welder required)
    Replies: 1
    Last Post: 11-01-2011, 07:38 PM
  4. Powder Coating Oven project
    By DAC45 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 10-13-2011, 04:18 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •