Share
Results 1 to 3 of 3

Thread: Project 1 from Welderdude, a walkway addition.

  1. #1

    Default Project 1 from Welderdude, a walkway addition.

    I had plans of posting some more projects, but haven't much time to work on anything. Anyways, I work at a waste water plant and get the chance to built stuff every now and then and had the chance to fab up a walkway addition to fill a dangerous gap between the original platform and the poo pressing machine as I call it. The gap had been there for years, but there was a 2 foot diameter pipe between the press and the steps, so it didn't seem as bad.



    I used 1.5 inch by 3/16 angle steel and cut a piece of scrap fiberglass grating. Its amazing how strong the grating is by its self.

    I used an old Solar ac only stick welder that runs on a whopping 200 volt instead of 230. 6011s are a pain to use with it, but 6013s still work.



    I used existing bolt holes because I didn't want to compromise the heavy zinc coating on the steel frame. It was a bit inconvenient, but ended up working out quite well.







    I sandblasted and used a heavy duty tractor paint hoping that it will last for a few years. That whole area gets exposed to some nasty stuff that eats paint like crazy.







    Overall, it worked out quite well and my boss was happy.



    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  2. #2

    Default

    The best paint for the metal on that would be Galvacon, wipe it down with lacquer thinner and brush on, dries in about 25 min and prevents rust very durable
    A good safety fix for an obvious hazard, wouldn't wanna fall there.

  3. #3

    Default

    Ill have to keep that in mind. I would of liked to use a 2 part paint made by Tnemec, but wasn't able to get any. It will last years in an anaerobic digester as long as you dont chip it. It would of been perfect because that press squeezes all the moisture out of the anaerobic digester sludge.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Similar Threads

  1. Project 2 from welderdude: custom tv wall mount.
    By welderdude in forum Other Custom Fabrications
    Replies: 9
    Last Post: 02-25-2012, 06:45 PM
  2. Project #1 from welderdude: parting tool holder
    By welderdude in forum Other Custom Fabrications
    Replies: 0
    Last Post: 01-27-2012, 02:42 AM
  3. Project 5 from Worntorn -4 stalls , tack up aisle + Hay loft Barn Addition
    By worntorn in forum Personal Projects (no welder required)
    Replies: 2
    Last Post: 06-12-2011, 11:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •