    First I am not much of a tig welder so I would not judge the machine by my lack of ability. This is the first time I have ever used a scratch start tig. This is a header that my friend Reed needed welding. This is a temporary fix until his new headers arrive. It seems about the time I get better at tig welding it's a month before I use it again. The Power Arc 140st is a very handy machine. I was very impressed welding at 25-30 amps, and I liked using the scratch start better than I thought I would.







    This is the first hole I have filled with a tig, I got the hang of it after I filled in this one. A little too much build up.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Sean, I thought that the 140ST was Lift Arc rather than scratch start. Lift Arc initiates the arc after sensing contact made between the tungsten and workpiece has been broken. It only uses a sensing voltage rather than the full voltage, full current of scratch start.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

Similar Threads

  1. Analog 200dx only welds in mma, no power in tig mode
    By airride in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 07-30-2013, 04:19 AM
  2. My first welds with my PA 160 STH
    By ironmanjay in forum Stick Welding (SMAW)
    Replies: 9
    Last Post: 07-25-2013, 04:23 PM
  3. My Welds
    By Oxide00 in forum Other Custom Fabrications
    Replies: 35
    Last Post: 11-09-2011, 12:23 PM
  4. how are my welds
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 05-20-2011, 02:46 AM
  5. First welds
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-07-2011, 07:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •