I ordered 25' torch with my PP256. The welder showed up with the standard blue handled 15' wp18 torch. This is the euro style torch and it's quite big.

The 25' torch arrived a couple of days later. It is marked SR20 , which I imagine correlates to WP 20. It is similar in size to a wp9 air cooled, so nice and compact, just like the torches in Mark's recent post. As Mark said there would be, it has a switch on it. This is just a little plastic switch zap strapped on. At first I planned to remove the switch in order to make the torch a bit less bulky, however I find the switch provides a good finger grip on top when the torch is held from underneath like a pencil.

Also. the switch can come in handy now and then for tacking things in difficult spots. So it'll stay for now.

I might put a short piece of large heat shrink on the torch handle to outer sheath connection. Right now that is done with electrical tape, that looks like it won't last very long.

What is the amperage rating for this small torch (with cooler in use)?

This is a rigid torch and there was no flex neck in the package. Is a flex neck available for this torch?

Glen