Share
Results 1 to 6 of 6

Thread: Anyone using the 205P or 250P?

  1. #1

    Default Anyone using the 205P or 250P?

    I have a Hobart Handler 210 and it is a nice machine. I have been reading about PULSE MIG lately and the advantages of using it for welding aluminum. I'm giving some serious consideration to getting a bit more powerful machine. Maybe Pulse mig.

    I've been getting a lot of aluminum work lately and although I like my Hobart with the spool gun, it does have a lot heat generated and I have had situations where even though I have it dialed in, the edges of some of the projects have melted pretty bad where in the areas away from the edges look great.

    I've seen some of the older posts about the pulse migs...but usually with the response that they rarely use the pulse option.

    Questions are:

    Is it worth getting the pulse mig?

    What other advantages does pulse offer over standard mig?

    How's the Everlast units as far as reliability?

    Any other things I should know about?
    Last edited by Steve; 08-30-2011 at 01:40 AM.

  2. #2

    Default

    The 250P yes, it is worth it. The 205P just doesn't generate enough power to spray...which is part of the point...Of course you can pulse short circuit, but it can lead to incomplete fusion if not done properly. The 250P have been very reliable. We rarely have a problem with a MIG... The new units also feature stick welding and spool gun port as well as an "OFF" switch for pulse so it can be used as a standard welder.

  3. #3

    Default

    Just my opinion, but since you have a nice mig welder, why not add a tig welder to the collection? I will admit that I'm saving up for a 250p I got a 50% off coupon for the last contest. I moved a month ago and have had a harder time getting welding jobs.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    Just my opinion, but since you have a nice mig welder, why not add a tig welder to the collection? I will admit that I'm saving up for a 250p I got a 50% off coupon for the last contest. I moved a month ago and have had a harder time getting welding jobs.
    I already have done that. I've got a Powertig 250EX and use it a lot. I've seen some of the advantages of pulse mig and am impressed with the ability to weld aluminum with the process. The Powertig 250EX welds aluminum just great but is slow.

    If you are looking to get a welding job, you might try North Dakota. The oil boom up there is helping keep their unemployment rate around 4%. But the biggest thing they have going for them is that they have their own state run bank. All the money and profits from state economic activity is kept in North Dakota and not sent to NY and Wall Street. That is allowing them to keep their money and create jobs. They have jobs available and need welders there from what I have heard.

  5. #5

    Default

    Quote Originally Posted by performance View Post
    The 250P yes, it is worth it. The 205P just doesn't generate enough power to spray...which is part of the point...Of course you can pulse short circuit, but it can lead to incomplete fusion if not done properly. The 250P have been very reliable. We rarely have a problem with a MIG... The new units also feature stick welding and spool gun port as well as an "OFF" switch for pulse so it can be used as a standard welder.
    Gotta argue about the 205/205P not being able to spray. According the the attached site, they are capable of spray if you use the right gas.
    http://www.praxair.com/praxair.nsf/0/c56dbfa8e80d0dbd85256ab300140b28/$FILE/P-8126.pdf

  6. #6

    Default

    Quote Originally Posted by performance View Post
    The 250P yes, it is worth it. The 205P just doesn't generate enough power to spray...which is part of the point...Of course you can pulse short circuit, but it can lead to incomplete fusion if not done properly. The 250P have been very reliable. We rarely have a problem with a MIG... The new units also feature stick welding and spool gun port as well as an "OFF" switch for pulse so it can be used as a standard welder.
    I would only trade or sell my old old old style 250P for the new one. I have plenty of stick machines, never really needed the pulse all the way off off, and I have an IMIG-200 for most spool gun work, but it "would" save me some space.

    Also, for me to sell my 250P, it would have to be a local sale as it ships on a palette. It's a beefy thing, but a great welder.

    Mark was down years ago setting up a dealer South if me, when the 250P came in. He popped over to play with it. It will spray for sure.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. powerultra 205p ?
    By travis in forum Pre-sales, Sales and Shipping questions
    Replies: 0
    Last Post: 06-04-2013, 10:19 PM
  2. I-Mig 205 vs. I-Mig 205P
    By MuttonHawg in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 01-20-2013, 01:01 AM
  3. up in smoke PU 205p
    By sydneysdad in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 01-11-2012, 11:32 PM
  4. mig 205p
    By Ernie in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 01-08-2012, 02:20 PM
  5. 205p Mig
    By Ernie in forum Introduce Yourself