Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 21

Thread: Project 1 from I_Love_Plasma ~ Getting familiar with stick welding.

  1. #1

    Cool Project 1 from I_Love_Plasma ~ Getting familiar with stick welding.

    Remember, I am nowhere close to professional, I am still a green-horne.

    I need practice, encouragement, and tips. Thanks!

    Hmmm, nice AC buzz box..


    Oh joy ... bare wires


    Trip to Ace Hardware>>> K-T Industries Rods


    6011 running at 117Amps (recommended 80-125A) needs to be less than 117.
    ,


    Right 7018 at 117Amps (90-140) Could be hotter than 117.
    ,
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  2. #2

    Cool

    More: It only allows 10 pictures per post, and I believe smiles count as pictures to.

    7018 @ 117Amps
    ,


    Focus on top weld>>


    Decent swirls, not really uniform yet. Better than I was.
    ,


    Focus on the weld closest to the camera on the surface; Not side weld.


    The weld that starts at the end is 6011. Focus on the cap welds in the center of pic.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  3. #3

    Cool

    More:...

    The root pass was 6011. Everything else was 7018 capping re-weld.
    ,


    Focus on right portion of the top weld.. good swirls and good finishing bead puddle.


    Last weld of day; 11 rods total 9 went to good use, 2 fried. Looking much better than before. ,
    ,


    HAHA look what I found! An old air-horn off a crane! 136dB of pleasure



    Alright, let the commenting begin! Thank you very much in advance.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  4. #4

    Cool

    Here's a video of me welding.

    Go to the first post after watching and read your way up.

    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  5. Default

    Well your starting to improve, I can see that you have really been slowing down. Still have a few that your moving too fast and not steady. Need to work on the consistity of the welds but you have greatly improved. Keep on a practicing. Your getting there. Have some nice welds in there. Do you do a whip and pause or circles or what?
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  6. Default

    Ok im I just started the video and noticed that the first weld still needs to be slowed down. Also You need to pause for a second when you come back each time
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  7. Default

    O wait you aint doing step and pause. Circles. But looking good. Much better!
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  8. Default

    Them last welds were looking good. You had a good travel speed and it shows by how they looked. Keep on working on them. Keep getting welds that look like that and your ready to start on the quick detach project
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  9. #9

    Default

    Looks like you are on the right track of improvement. I read or heard some place that you should not hammer on the weld to get the slag off as it can cause the weld to crack. I learned to stick weld in high school and they taught us to lightly tap it and brush off the slag.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  10. #10

    Thumbs up

    Quote Originally Posted by bobwills View Post
    Them last welds were looking good. You had a good travel speed and it shows by how they looked. Keep on working on them. Keep getting welds that look like that and your ready to start on the quick detach project
    Thanks Gabe I need to get more uniform. And I still don't leave my ending puddle like I'm supposed to do. Pretty good video footage huh?

    Quote Originally Posted by Jason View Post
    Looks like you are on the right track of improvement. I read or heard some place that you should not hammer on the weld to get the slag off as it can cause the weld to crack. I learned to stick weld in high school and they taught us to lightly tap it and brush off the slag.
    Hmm, very good to have that in the knowledge arsenal. These were just practice welds and a lot of my welds had slag impregnated in them so I beat the flux out then brushed them (fast, I went so fast it was like buffing it LOL ). As my welds got better less slag was impregnated in them. I also have heard the same: "you're supposed to chip it off gently and brush or sandblast the rest."
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  11. Default

    Welcome. And yeah. Just the more practice you do the more uniform you will get. Another thing to work on is your starts still. You will get it all after a while. And yeah. Get ya like a #10 shade or something on the front and you can videotape the puddle.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  12. #12

    Default

    Oh yeah, I forgot to mention the starting. I was having a lot of problems with sticking because of the amperage. I did boost it up a bit. I could tap start 7018's then, and at 117amps I could tap a 6011 easily.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  13. #13

    Cool

    More pictures! Go ahead and critique my welds.

    Kinda blowing out still at the end...not leaving an end bead. 6011 at 97 amps Don't know where that seed came from lol


    Running to many amps for 6011 rods. Stringer beads. 117 amps


    haha got a little welding frost on my shield.


    All the rest are 7018 at 117 amps, might be a touch cold. But the slag chipped off in large chunks.


    Last edited by I_Love_Plasma; 09-26-2011 at 02:43 PM. Reason: Commented about the sunflower seed...weird lol
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  14. #14

    Post

    Here's a new video of me welding with AC.
    I am asking for tips and how-to's. The first part of the video you are viewing the welding, puddles, travel speed, etc... Second part of the video is the finished welds with most of the slag scraped/chipped lightly off and me talking about the welds.

    During the video I accidentally said the welds breaking sounded like a shotgun. It was more like a .22LR. Still scared the crap out of me being a foot away when this big noise pops at me.

    Oh yeah, I finally got smart and used a work table instead of the "monkey squat" as Mike R. calls it. lol


    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  15. Default

    first thing is that ya need a darker lense on the camera cause ya cant see the puddle through the camera lol. Just your getting there. Find your amps and juat keep working on it. Try to slow it down some still. Can see your maving around a lot. Also try to run full beeds. Not those little 1 or 2 second ones. That only will help you work on your starts. Try doing full rod beeds with no stops. It will help you the most. And what was some of that wide sweeps in there sometimes all about???
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  16. #16

    Post

    Well I was doing my overlapping circular whip motion and I decided to goof off and try a zig-zag...I was told to try it lol. He might have well just told me I need to replace my muffler bearings Zig-zagging makes welds look like the rod had rabies and a bee in it's eye.

    Pretty nice run with the 7018 huh?
    Last edited by I_Love_Plasma; 09-27-2011 at 12:51 AM.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  17. Default

    lol i think ya got a little out of controle with the zig-zags. ya were going way wide. And yeah not bad. Need to ge able to get a whole rods worth to look like that. Not just a part, but work on running full rods at a time. And need to get where you can make welds like that 75% of the time then your good to go.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  18. #18

    Default

    HAHA that was a perfection run for dad, he gets bored watching me weld I guess, so I stopped it short. He was impressed, which is rare. I will try running full rods. 7018's are my favorite rod. 6011's are okay for farmer welds. I was thinking Ill take the plasma and cut a straight line all the way down one piece. Do you steady your rod with your thumb when the rods long? I guess I'm going to have to practice the ole free hand method, because that's why I go a ways then stop. My gloves get pretty hot steadying.. What's your preferred method of holding?

    I hold the electrode like this in the gun (dots represent electrode, lines are the gun horizontal)

    _______________

    _______________. .
    ````````````````. .
    `````````````````. .
    ``````````````````. .
    ```````````````````. .
    ````````````````````. .
    `````````````````````. .
    ``````````````````````. .
    ```````````````````````. .
    Last edited by I_Love_Plasma; 09-27-2011 at 02:15 AM.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

  19. #19

    Default

    try stacking your bids one after the other and run longer beads. longer beads will help with your consistancy.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  20. Default

    Ok the way i hold the rod is on flat welds i put the holder in a 90 degree spot then i hold the holder in my right hand. Then put my left hand pinkey on the metal spread my thumb up far as it goes then rest my other hand on top of my thumb. It works the best for me. Its the way jody was showing in the arc welding vid that he was working on the pipe bender stand. It allows your hands to colapse together making the whole rod length comfortable for welding. Remember comfort is a key to getting good welds and consistancy. Then i do the 45 degree angle making a wider than 90 angle for verticle and prop my elbo for that with left hand around right hand which is grabbing the electrode holder. Just experement and find out what works best for you
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

Similar Threads

  1. PP50 arrived with familiar problem
    By keweenawbee in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 11-14-2012, 11:03 PM
  2. Project 4 from I_Love_Plasma ~ Slab Carrier Overhaul
    By I_Love_Plasma in forum Heavy Equipment and Commercial Projects
    Replies: 0
    Last Post: 10-25-2011, 02:47 AM
  3. Project 2 from I_Love_Plasma ~ Custom Mulch Bucket
    By I_Love_Plasma in forum Heavy Equipment and Commercial Projects
    Replies: 15
    Last Post: 10-08-2011, 07:23 AM
  4. Project 3 from I_Love_Plasma ~ Parts/Firewood Dump Box
    By I_Love_Plasma in forum Heavy Equipment and Commercial Projects
    Replies: 0
    Last Post: 10-04-2011, 07:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •