I'm the half owner of a SuperCut 50. We've actually cut like 1.125" steel before with it! Of course it wasn't a very pretty cut...But it did it! Makes great cuts when you are cutting the recommended thickness. I'd have to give it a 5/5 rating.
I'm the half owner of a SuperCut 50. We've actually cut like 1.125" steel before with it! Of course it wasn't a very pretty cut...But it did it! Makes great cuts when you are cutting the recommended thickness. I'd have to give it a 5/5 rating.
Benjamin
Owner of IMIG 200 and half owner of Power Plasma 50