I was working doing some work on my duck boat when I ran into a problem. I was only getting the HF arc, it would never ramp up to the full arc. I also noticed that the amps on the display said 205 when I had set it to 125. I had started out at AC, 125amps balance at 20% and ac freq 110 -120 , up and down slope set to zero and the pre and post flow set at about 2 and no pulse with the peddle and it 2t mode. The machine was working just fine for the first 4 welds. Then on the 5th I just got the HF arc, so I moved the ground clamp to try and get a better ground that still didn't help. So I got out of the boat and noticed the amp display was at 205 and the lowest it would go was 130. So I got clean steel bar and put the clamp on it and tried to get the arc going and still just the HF arc. I tried calling support but there are not there yet and couldn't leave a message. Anyone have this problem and how did you fix it?

I also tried switching to DC but I got the same results.