Thread: Project #3 from Hooda- Electrolytic rust removal EXPERIMENT!

  1. #21
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    That's awesome. Thanks for the time and effort you took to experiment and refine the process, it makes me wish I had something rusty (and a battery charger) to try this with. Maybe I'll have to try it with an old computer power supply.

    I think your observations/theories on the anode are probably correct, a more uniform current density certainly wouldn't hurt anything and rinsing the sponge and resoaking it with fresh electrolyte will eventually be necessary.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  2. #22
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Just a reminder: Hooda used a sponge as a workaround because the jointer was too large to put in a vat. The ideal situation is to immerse the rusty part and the anode in the electrolyte fluid.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

Similar Threads

  1. Project 2-5 From Hooda- Engin stand mod for HD use.
    By hooda in forum Personal Projects (no welder required)
    Replies: 6
    Last Post: 02-26-2012, 09:31 PM
  2. Project #2-3 From Hooda-Caravan engine rehab
    By hooda in forum Personal Projects (no welder required)
    Replies: 4
    Last Post: 02-17-2012, 03:58 AM
  3. Project #1-3 Form Hooda-Snowblower modification
    By hooda in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 12-25-2011, 07:37 PM
  4. Project 3 from ogorir: floorpan/firewall rust repair
    By ogorir in forum On Road Fabrication
    Replies: 5
    Last Post: 10-25-2011, 04:48 AM
  5. Project 1 from DaveO: electrolytic rust removal
    By DaveO in forum Personal Projects (no welder required)
    Replies: 15
    Last Post: 10-13-2011, 03:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •