What is the proper way to cut expanded with the pp50 without hurting it? Thanks
What is the proper way to cut expanded with the pp50 without hurting it? Thanks
Last edited by trickbiker; 10-18-2011 at 11:46 PM.
Trickbiker
I would lean towards 3 inch cutoff wheel myself. Plasma seems like over kill. Just my thought.
Mickey,
Well if you leave the torch on unnecessarily you'll shorten the life of you consumables..you probably already know that, just thought I'd mention it just as an FYI. Are you worried about hurting the machine?
I think what I would do is get a straight edge. I think your unit should have a pilot arc so the flame/arc stays lit/burning.?? Correct me if I'm wrong. Take your straight edge and clamp it at both ends, then take your torch using one hand to slide on the straight edge and your other hand to switch and hold the torch. Just set your height above your expanded metal and just leave the trigger squeezed. Just drag it toward yourself using a moderate speed while cutting then quick hops between the gaps.
Hope this helps you or at least gives you a starter idea,
ILP
I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.
http://brothers2woodworking.webstarts.com/
Everlast Plasma cutter Power Plasma 50
Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.
Wishlist: Free consumables, Small TIG maybeAlex, when you have overstock give me ring!
Here's a video of Performace (Mark) cutting expanded metal with the PP60 which should work the same...
youtube is a little slow to respond right now so give it a minute if the video doesn't show.
Last edited by zoama; 10-19-2011 at 03:36 AM.
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
Last edited by trickbiker; 10-19-2011 at 03:51 PM. Reason: to correct my statement
Trickbiker
Thanks for sharing that video, that's just what I was looking to do too.