I'd like to weld stainless(304) v-band flanges on the exhaust manifolds of the 2-stroke saabs I work on for better sealing and easier disconnect. I've only welded mild to cast iron or cast iron to itself, any thoughts? because 'cast' rod is mostly nickel anyway (55 or 99%) I can't see much of a problem using a high-nickel stick rod, but I figure I'll solicit opinions anyway.

this is also probably thick enough that I can TIG it with the I-MIG, though, so if anyone has a dynamite TIG filler for welding 304 stainless to highly carbon-impregnated cast iron, I'm all for it