    Everlast,

    I noticed this statement on your homepage "Our Everlast Welders and Plasma Cutters now come standard with Siemens IGBT technology from Germany to ensure the highest quality product available.".

    But the specs on the SuperCut40 and SuperCut50 state "Mosfet Technology with Fuji or Toshiba Mosfets".

    Which statement is true?

    Thanks,
    Mark

  2. #2

    Default

    Well first off, all of our products are quality products. MOSFET or IGBT. The product design and brand of the parts inside are the key.

    We have "two" units that are MOSFET in our large line of plasma cutters and welders and it is stated on the website as you point out.

    The MOSFET unit price is lower and the duty cycle is as well. These are for people getting started in welding/cutting on a budget.

    What are you looking to do? We can help find you a unit that will fit your needs.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. Question

    I don't mean to argue but your statement about the duty cycle does not seem to be correct either.

    From the "SuperCut 50" (IGBT) Spec. Page.
    "Power Specs:
    Power Factor 0.93
    100% Duty cycle (cut time) at 40amp cut
    60% Duty cycle at 50amp cut setting"


    From the "PowerPlasma 50" (MOSFET) Spec. Page.
    Power Specs:
    Power Factor 0.93
    100% Duty cycle (cut time) at 40amp cut
    60% Duty cycle at 50amp cut setting


    Thanks,
    Mark

  4. #4

    Default

    Tex,
    Both are true. The front page was slightly edited for length and the original statement may have gotten the axe about the "baby" unit.
    The mofset units do contain some IGBT technology, albeit in another part of the unit.

    It is the one "price" machine that we carry with Mofsets. For now we have decided to stick primarily with IGBT powered welders.

    Our PowerPlasma units are IGBT...Our SuperCuts are Mofset. You got it reversed.

    But other than that, you are correct. 60% duty cycle at 50 amps.

  5. Default

    Thanks for clearing this up.

  6. #6

    Default

    It seems I can't spell MOSFET correctly either at 3 in the a.m.
    lol

  7. Default

    Hey joejoe, welcome, and take a look at a thread I started "need help picking out a plasma cutter" The fine folks at everlast support have answered that question.
    Miller Dialarc 250
    ESAB Migmaster250
    Smith Heavy Duty OXY/ACETYLENE outfit
    Arcair gouging set

  8. #8

    Default

    I was wondering if I buy an everlast plasma cutter, will i be able to use it in both manual and mechanized cutting. And does anyone do this now thanks Joe

  9. #9
    Join Date
    Apr 2011
    Location
    Sasktachewan, Canada
    Posts
    95

    Default

    Here are two really good videos about the differences between Everlast MOSFET and IGBT plasma cutters. They may help in your decision.

    http://www.youtube.com/watch?v=665Zu1hHbag

    http://www.youtube.com/watch?v=Prbf-...eature=related
    Attitude Determines Altitude

  10. #10
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default Why the difference in IGBT vs MOSFET?

    I'm officially sold on EVERLAST (have been for some time), and officially sold on IGBT. The next question is why the disparity in cut quality between the 2 machines? I think that someone making a decision based JUST on the 2 you tube videos posted before me would be scared away from the MOSFET unit. My assumption is that the MOSFET machine cuts much better when the material is down in the 1/8" Yes? No?
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  11. Default

    The IGBT does cut better in all rated thicknesses compared to the Mosfett Units. In addition there are a number of differences in the build of the unit besides the obvious Inverter Technology .
    As for cutting Quality in the thinner cuts , i find this difficult to tell them apart but you also need to keep in mind we are talking fairly thin material.
    With 1/4 and 3/8" as a example ( these are the sizes i use for testing units ) The IGBT will be set at 24 -25 amps and the mosfett 35 amps for 1/4" on 3/8 it is 35 compared to 45 amps
    I do this to get a close quality cut for both units but i do see the IGBT being a little cleaner.
    I have mentioned this in another post. But the quality of the newer models will exceed the past products due to the better quality Plasma Torch being used.
    If i can get some time over the next 2 days to do some pictures or videos this will be very apparent . I am a little pressed for time right now as i am scheduled back at the factory and will be leaving Thursday morning. I may not personally be able to do this but i can see what can be done in my absence.
    I will try to also post up some pictures showing the new 25 amp 110v plasma while at the factory
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  12. #12

    Default

    I have a dumb question... I have a lotos cut50 I bought off Ebay. I can't complain because it cost me $300.00, but there will come a time soon I hope when I get a better plasma cutter. It does not have the pilot arc is that a difference between Mosfett and IGBT?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  13. Default

    Quote Originally Posted by SeanMurphy265 View Post
    I have a dumb question... I have a lotos cut50 I bought off Ebay. I can't complain because it cost me $300.00, but there will come a time soon I hope when I get a better plasma cutter. It does not have the pilot arc is that a difference between Mosfett and IGBT?
    No it does not mean that Mosfett can not have pilot arc start. In Fact our Supercut 50 is primarily a mosfet Inverter although the Control for Pilot start is IGBT.
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

Similar Threads

  1. IGBT vs MOSFET?
    By The Tig Kid in forum General Welder Questions
    Replies: 1
    Last Post: 02-19-2014, 10:03 PM
  2. supercut 50 igbt not cutting
    By zinger in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 02-01-2012, 09:43 PM
  3. IGBT vs MOSFET
    By bobwills in forum Everlast Plasma Cutters (PAC)
    Replies: 17
    Last Post: 10-12-2011, 01:55 PM
  4. IGBT Question. Couldn't believe what I just saw
    By hooda in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 04-12-2011, 03:27 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •