I when to try out the LX and when I try to weld I get the Cup getting red hot and lots of electrode wear

set on DC Neg electrode id I have pos to the electrode it melted the tip with in seconds
amps the red knot less than 100 around 80. Tig amps at about 9 o'clock gas at 15 using the hand trigger welding mild steel less than 1/4 plate

if I use 4 T it takes longer for it to happen but still did do it

Also noted at 1st I could not get my gass flow to come off zero had to DC it from the unit then it worked fine after reconnect anyone got any links to pics on dial setting
oh it was a number 20 torch with water cooling and a using the only cup they sent with it a #4