Share
Results 1 to 12 of 12

Thread: New Power Pro 256 Problems or User?

  1. Default New Power Pro 256 Problems or User?

    Just hooked up new Powerpro 256. I'm trying out the plasma cutter and even turned all the way up it wont cut 3/8. I have good power and plenty of air. I've tried several settings on pressure. I've tried with standoff and without and tried different consumables. Any Ideas? Everlast isn't open today and I'm out of town for the next few days.

  2. #2

    Default

    Yes,
    You can call in on the weekends and leave a message, and you may get a return call anyway, or at least get in line for one for Monday.

    The standoff should be less than 1/8" and closer if you can.

    What was your psi?

    I assume you had it turned up? Is the torch in the negative?

    What about your work clamp?

  3. Default

    I don't have such a machine, but I can throw out some ideas...
    Is the work clamp connection good? Switch on machine set to plasma?
    Is the work clamp in the (+) connector and plasma torch in the (-) connector?

    eta... beat by 4 minutes!

  4. Default

    Work clamp is good, Torch in -, clamp in +, and I've tried from 40 - 60 psi

  5. #5

    Default

    Quote Originally Posted by mwbmd11 View Post
    Work clamp is good, Torch in -, clamp in +, and I've tried from 40 - 60 psi
    Do you get a pilot arc when you press the torch button ? (torch away from the work piece)
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6

    Default

    Quote Originally Posted by mwbmd11 View Post
    Just hooked up new Powerpro 256. I'm trying out the plasma cutter and even turned all the way up it wont cut 3/8. I have good power and plenty of air. I've tried several settings on pressure. I've tried with standoff and without and tried different consumables. Any Ideas? Everlast isn't open today and I'm out of town for the next few days.

    mwbmd11
    you may need 1.0 tips ,(you have 1.2mm now) we have them and i can send you pack for free.
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  7. Default

    i got it! It was a loose connection where the torch is attached at the unit. Still seems a little slow. I would like to try the 1.0 tips.
    Last edited by mwbmd11; 11-21-2011 at 02:58 AM.

  8. #8

    Default

    The 1mm tips will give you a smaller kerf, but limit your amps so if you get some, note they are best on thinner sheet. The 1.2mm will cut sheet metal fine, you just want dry air, a guide (when possible) and move at a good constant speed.

    Also, we cover the forum and some of the techs return calls on the weekend as well as from the forum.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  9. Default

    What amp range is appropriate for the 1.0mm and 1.2mm nozzles?

  10. #10

    Default

    1mm and 1.2mm are very close so the amps will be about the same (20-60 amp should be fine), but again, depends on the person moving the torch as well, and dry air will make the consumable last longer..
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  11. Default

    OK, thanks.
    I had the impression that the 1.2mm was for ~80 amps.
    The 1.2mm is 20% larger diameter than the 1.0mm, and 44% more area.
    Last edited by parkour; 11-21-2011 at 09:01 PM.

  12. #12

    Default

    Not to hi-jack this thread but..

    I think some go up to 6 or 7mm and probably higher. The 1.2mm can be used on an 80 amp. Next time I talk to the Trafimet rep will try to remember to ask, but sure he will say there is no set number just a range. Like welding, no two guys seem to ever be the same, just close.

    I have A81 swirl rings and nozzles on order so probably soon (after Thanksgiving).
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. power arc 140st problems
    By fitter in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 09-07-2013, 10:36 PM
  2. First run (with some problems) - Power Tig 225lx
    By marcio in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 03-14-2013, 01:26 AM
  3. User Request: User Customizable Skins for the forum
    By Spike in forum Forum related Questions
    Replies: 3
    Last Post: 01-24-2013, 01:50 PM
  4. Problems with Power Plasma 50
    By Mattox in forum Everlast Plasma Cutters (PAC)
    Replies: 0
    Last Post: 11-02-2010, 05:49 PM
  5. Power Master 205 New User Review
    By 91TSiGuy in forum Customer Testimonials
    Replies: 6
    Last Post: 03-12-2010, 04:43 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •