Share
Results 1 to 13 of 13

Thread: My best welding so far... Aluminum... Pic

  1. #1

    Default My best welding so far... Aluminum... Pic

    I've been welding Aluminum for the last few weeks in night school and I'm finally feeling "comfortable" while welding it. My inside corner welds are getting better but I still need some time with those.
    This box was welded with my Everlast 250EX 30 mins. ago...


  2. #2
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Thats purdy, I hope I can get that good. How thick was the stock?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  3. #3

    Default

    11 gauge (1/8")

    I've been welding for about 3 weeks on Aluminum 3 nights a week. I've got about 20 hours in practice at school and maybe 3 hours or so on my 250EX

  4. Default

    That looks nice. Is it air tight?
    The one time I tried to weld something air tight... it didn't work well.

  5. #5

    Default

    yes. You just gotta go slow at the last open area because of the pressure inside it. First time I did one of these it was like "Kapooof!" Blew out a big hole and made a mess.....I learned on that one!

  6. #6
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Nice weld, that is a consistent bead for a free-hand weld.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  7. #7

    Default

    Thanks! That's what I'm wanting/trying for, a nice consistent weld bead.
    I went to Tractor Supply the other day and they are selling Aluminum truck tool boxes for cheap.... The weld, Honestly, looked like someone just held the torch close, moved it along and melted the two halves together. Didn't look good at all.

  8. #8

    Default

    Like you said cheap.
    When you pay peanuts you get monkeys.
    Good welders don’t come cheap

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  9. #9

    Default

    Quote Originally Posted by CGCINC View Post
    Thanks! That's what I'm wanting/trying for, a nice consistent weld bead.
    I went to Tractor Supply the other day and they are selling Aluminum truck tool boxes for cheap.... The weld, Honestly, looked like someone just held the torch close, moved it along and melted the two halves together. Didn't look good at all.
    Nice welds on your box, the truck boxes were probably mig welded not too many fab guys would use tig on such items.
    Some of those lies people tell about me, are true

  10. #10

    Default

    Quote Originally Posted by CGCINC View Post
    Thanks! That's what I'm wanting/trying for, a nice consistent weld bead.
    I went to Tractor Supply the other day and they are selling Aluminum truck tool boxes for cheap.... The weld, Honestly, looked like someone just held the torch close, moved it along and melted the two halves together. Didn't look good at all.
    Those boxes are mig welded. The welds are often sloppy but they do hold the boxes together.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  11. #11

    Default

    Quote Originally Posted by Steve View Post
    Those boxes are mig welded. The welds are often sloppy but they do hold the boxes together.
    The box I looked at was not Mig, Tig or Stick welded, it was melted with a torch, lol.... I've Mig'd Alum. with a spool gun at class and I still had the "bead" look after welding so it must have been the guys first day on the job!
    I guess you would need to Mig it when in production, Tig would take forever for one of them.

  12. #12

    Default

    Verry nice.

    Regards: M J Mauer, Andover, Ohio

  13. #13

    Default

    Quote Originally Posted by CGCINC View Post
    yes. You just gotta go slow at the last open area because of the pressure inside it. First time I did one of these it was like "Kapooof!" Blew out a big hole and made a mess.....I learned on that one!
    Welds look great! Nice work.

    One tip that usually works on a sealed weld is to actually weld 75% of the box, then drill a `1/8" hols in the corner of one of the completed welds to act as a vent. finish up all of the welds, then let the item cool. Go back and fill the hole. The cool box and cool air tends to take a little time to expand and doesn't build as much pressure as quickly. Depending on the size of the part, sometimes this does no work due to the part heating very rapidly and the air expanding very quickly anyway. Could probably also just leave a 1/4" or so at the end of one of the welds, let it cool and come back to save on drilling / filling.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. aluminum welding with mig
    By rebelbah in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 10-18-2016, 04:36 PM
  2. mig welding aluminum
    By Rodsmachineshop in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 06-20-2012, 11:50 AM
  3. tig welding aluminum with a DC only tig
    By rab in forum General Welder Questions
    Replies: 18
    Last Post: 04-03-2012, 02:25 AM
  4. Replies: 2
    Last Post: 08-03-2011, 03:50 PM
  5. Tig welding aluminum
    By Tallguy64 in forum General Welding Questions
    Replies: 6
    Last Post: 04-10-2010, 11:02 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •