    I did a little repair work for my church Monday. I welded a piece of stainless on our hot plate (buffet table), that holds the glass. I can't say that I have ever welded any stainless. It blacked up on me pretty good, and after I got the hang of it I put down an ok bead. I was using 2% thorated tungsten and 3/32 rods. I know I needed thinner rods. No one keeps any stainless rods in stock, I bought 3 pieces at a local machine shop. The guy asked me what alloy I was welding on. I told him I had no clue, and I was just supporting a piece of plexi glass. My questions are

    What do I need to do so the metal will not black up?
    Do I need different rods for different stainless?
    Is there a good middle of the road stainless?
    What tungsten should I use?
    Is there a certain way I should hold the torch?

    By the way I was using my handy dandy Power Arc 140 ST
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    I did a little repair work for my church Monday. I welded a piece of stainless on our hot plate (buffet table), that holds the glass. I can't say that I have ever welded any stainless. It blacked up on me pretty good, and after I got the hang of it I put down an ok bead. I was using 2% thorated tungsten and 3/32 rods. I know I needed thinner rods. No one keeps any stainless rods in stock, I bought 3 pieces at a local machine shop. The guy asked me what alloy I was welding on. I told him I had no clue, and I was just supporting a piece of plexi glass. My questions are

    What do I need to do so the metal will not black up?
    Do I need different rods for different stainless?
    Is there a good middle of the road stainless?
    What tungsten should I use?
    Is there a certain way I should hold the torch?

    By the way I was using my handy dandy Power Arc 140 ST
    You need a larger cup and higher argon flow for stainless.
    1/16 308L filler should be good for food service stainless which is usually 304 or 316.
    !/16 2% thoriated will work, if you only have 3/32 then grind it to a finer point.
    Hold your torch the same 85 degrees and 15 degrees for the filler rod.

    Stainless holds heat so your work can overheat if you try to weld too much at once.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    [QUOTE=zoama585;18513]You need a larger cup and higher argon flow for stainless.
    QUOTE]

    I was wondering if this might be a shielding gas problem. Doesn the black appear on the top surface by the weld, and does it scrape or brush off? I recall a while back there was a discussion of back-ourging stainless steel tubing to prevent black oxidation on the underside of the weld, but this is different.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  4. #4

    Default

    [QUOTE=DaveO;18514]
    Quote Originally Posted by zoama585 View Post
    You need a larger cup and higher argon flow for stainless.
    QUOTE]

    I was wondering if this might be a shielding gas problem. Doesn the black appear on the top surface by the weld, and does it scrape or brush off? I recall a while back there was a discussion of back-ourging stainless steel tubing to prevent black oxidation on the underside of the weld, but this is different.
    Just about any metal will soot up without sufficiant shielding gas. For stainless to remain "stainless" in needs good shielding. You can checkout some stainless welding videos at weldingtipsandtricks.comr on youtube.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5

    Default

    Before feeling too bad about it, restaurant equipment is hard to weld, particularly used stuff because it is usually deposited with layers of grease or residue and it will black up...If it was used occasionally, maybe not, but anything that sees food service regularly get nasty to weld.

  6. #6
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    That's funny- I would have thought that manually cleaning and brushing beforehand would clear that up. Other posts have talked about using acetone, for instance, to pre-clean aluminum for welding... is it the same for stainless? Does the black crud come off? Seems like black stains would make the food way less appealing.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  7. #7

    Default

    the black stuff cleaned up easy, I used 3/32 2%thorated, and the point was dull. I can't remember what cup size I am using.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. Some stainless practice
    By redstopgreen in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 01-22-2014, 04:55 PM
  2. Stainless to low carbon, 309 or fab the other part from stainless?
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 07-20-2012, 05:07 PM
  3. 6G stainless
    By Oxide00 in forum Other Custom Fabrications
    Replies: 2
    Last Post: 03-22-2011, 09:41 PM
  4. Stainless filler?
    By Nikola Tesla in forum General Welder Questions
    Replies: 1
    Last Post: 03-22-2011, 04:57 PM
  5. Using AC on Stainless question
    By jtybt in forum General Welding Questions
    Replies: 2
    Last Post: 03-03-2010, 12:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •