    Default CGCINC Project #1 Welding table ... Lots of PICS!

    This is my small welding table.
    It's made out of 2.5" x 2.5" for the lower frame and for the upper frame and angled legs, I used 2" x 2". The top is 33" x 48", 1/2" plate. The 5" locking wheels I bought from NorthernTool for $8.99 each. They support up to 220lbs. each and they work great, the lock on the wheels is much better than the $29ea. wheels I saw at the local Tractor Supply. The adjustable/removeable standing station slides into the front 2.5" tubing and there is a locking bolt on the side to keep it in place.
    It turned out nice and I really like everything about it. The only thing not done yet is a removeable splash sheild for the back. I will be making it removeable so it's not in my way when I roll the table out in the middle of my shop.







    Grounding tab...



    Clamp hanger...



    Adjustable standing station...











    Foot pedal basket...
    Last edited by performance; 12-08-2011 at 04:40 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Project#3 from CGCINC. Category: General Welding Repair
    By CGCINC in forum Welding Repairs
    Replies: 5
    Last Post: 12-11-2012, 07:33 PM
  2. Project 1 from CGCINC. Category: Welding Cart
    By CGCINC in forum Other Custom Fabrications
    Replies: 20
    Last Post: 11-30-2012, 10:05 PM
  3. CGCINC Project#3: 1000lb. water fountain Many, Many pics
    By CGCINC in forum Personal Projects (no welder required)
    Replies: 28
    Last Post: 05-09-2012, 05:22 AM
  4. Project 1 from CGCINC. Category: MIG Welding Cart
    By CGCINC in forum Hobyist Projects
    Replies: 28
    Last Post: 04-12-2012, 09:21 PM
  5. bike build (lots of pics)
    By whitehendrix in forum Personal Projects (no welder required)
    Replies: 15
    Last Post: 03-13-2011, 05:57 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •