    I will be TIG welding some stainless rod to mild Steel plate. I'm just not sure what filler rod to use?

    I have 308L filler but a friend told me he would use 309L?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    sorry, 304 Stainless to Mild Steel
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    The 309L is preferred when welding a low 300-series to mild steel.
    Last edited by sportbike; 01-28-2012 at 09:21 PM.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4

    Default

    Alrighty, thanks!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  5. #5

    Default

    As important as the filler rod, is the process used. The stainless and mild steel will absorb heat at different rates, and will also expand and contract at different rates. Stainless to Mild Steel is prone to cracking if not done correctly. It's important to preheat both metals, and to 'ease into' the welding puddle. Don't just hammer down on the pedal and start the weld puddle, use light heat and make a little circle to warm up the puddle area and gently bring the metals to a welding puddle, then weld slower, and don't pour on the heat like is normally done with steel. After welding, let up on the pedal slowly, and post heat the weld area, and turn your post gas way up to keep the argon flowing over the weld.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

Similar Threads

  1. Welding 1/8 to 3/16 mild steel with powerarc 140st on 120v ?
    By ridenlow559 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-15-2015, 02:58 AM
  2. tig welding stainless help.
    By steve1989 in forum General Welding Questions
    Replies: 4
    Last Post: 02-13-2014, 06:22 PM
  3. Filler metal selection for welding mild steel and 4130 tube
    By hooda in forum General Welding Questions
    Replies: 11
    Last Post: 03-21-2013, 08:38 PM
  4. MIG welding stainless w/ C25?
    By EmptyNester in forum General Welding Questions
    Replies: 8
    Last Post: 08-31-2012, 01:30 AM
  5. stainless tig welding
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 08-27-2012, 07:20 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •