Share
Results 1 to 17 of 17

Thread: pp256 spark in front of panel

Threaded View

charger891 pp256 spark in front of panel 12-19-2011, 12:59 PM
performance That's the HF jumping. Don't... 12-19-2011, 03:18 PM
charger891 called in yesterday, took the... 12-20-2011, 03:37 PM
charger891 http://i925.photobucket.com/al... 12-20-2011, 06:17 PM
charger891 I`ll try it tonight, need the... 12-23-2011, 04:26 PM
charger891 took the handle apart, the... 12-23-2011, 01:00 PM
performance Did you try it while pressing... 12-23-2011, 02:54 PM
charger891 the other end of the yellow... 12-20-2011, 06:18 PM
Ray Charger, I can’t see the... 12-20-2011, 07:19 PM
charger891 Ray, it is imposible to... 12-21-2011, 01:08 PM
performance It may not be a ground issue.... 12-21-2011, 02:54 PM
charger891 Definately seems to be coming... 12-21-2011, 03:50 PM
charger891 Oleg, i tried e-mailing you... 12-24-2011, 06:51 PM
charger891 Yep, my pilot arc was also... 12-22-2011, 05:41 PM
Previous Post Previous Post   Next Post Next Post
  1. #1

    Default pp256 spark in front of panel

    finally had a bit of time this weekend to do some welding, only the second time i get to use this machine, set up the tig, open up the regulator, just going to purge my line, regulator wasen`t working, was just going to tap on like i dod last time and noticed a nice bright spark coming from the tig switch plug in to a bolt on the side panel, so i imediately checked the connection and removed and re-installed it and as soon as i hit the trigger on the torch i get this spark, WTF!!!

    http://i925.photobucket.com/albums/a...1/IMG_0149.jpg
    Last edited by charger891; 12-19-2011 at 01:03 PM.

Similar Threads

  1. Spark Container
    By Gerry in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 12-10-2012, 06:50 PM
  2. Spark Gap Contacts
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 28
    Last Post: 10-03-2012, 12:50 AM
  3. Front panel issue...
    By millermatic in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 08-28-2012, 03:07 AM
  4. Got a spark, but no cut, not an Everlast unit though.
    By CSR in forum Everlast Plasma Cutters (PAC)
    Replies: 24
    Last Post: 09-08-2010, 04:14 PM
  5. The Plasma air pressure low sensor on the front panel
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 1
    Last Post: 12-21-2009, 11:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •