Share
Page 1 of 5 123 ... LastLast
Results 1 to 20 of 92

Thread: Foot Pedal Issue

  1. Default Foot Pedal Issue

    I bought a Powertig 200LX here a while back. Its been working fine but this past weekend I was doing some welding. During a series of small tacks the machine started making a buzzing noise and would not strike an arc. I tried different tunsten, checked my argon, switched the machine on an off and it didn't change. Then I cranked up the knob on the pedal to max and tried and it would strike an arc but it was very weak. I had a friend strike an arc and I looked at the machine and it would only show 86 amps. I did switch back to the torch trigger and adjusted the amperage via the panel and it worked perfectly. That lead me to believe that there was something going on in the pedal.

    My assumption was that maybe the cog belt slipped on the pulley for the potentiometer inside the pedal? Does that seem like a possibility? I pulled the cover off the pedal and it looks ok, nothing loose or broken. The spring is still on the belt. Should I pull the belt off and rotate the pot one way or the other to see if its in the correct position (with the pedal fully off or fully on)? I'm just looking for suggestions on what to do to fix the problem or at least trouble shoot it.


    Thanks,
    Chris
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  2. #2
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default


    That would be a very good place to start, if that doesn’twork, give us a call and we can have you check the pot itself.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  3. #3

    Default

    Make sure you have your unit switched firmly into 2T.

  4. Default

    I'll head out into the shop here in a bit and play around with it. Thanks for the quick response.

    Chris
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  5. Default

    Did some checking last night. The switch was definitely in the 2T position. I took the pedal apart and pulled off the belt and operated the pot by hand and it still would not strike an arc. I went back to the trigger on the torch and it worked fine. I reinstalled the belt (which had not slipped BTW) and put the pedal back together and went to test it again and all of the sudden it was back to working just fine. I welded some scraps of steel and aluminum for about 20 minutes and it worked fine. Not sure what the problem was but it seems gone for the time being.

    Chris
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  6. #6
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default


    Huh, weird.



    Might want to check the solder connections on the pot?
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  7. #7

    Default

    Might have been an issue with the foot switch too.

  8. Default

    This weekend I have a bunch of chrome moly welding and a bit of aluminum welding to do. I'll give it a good workout. If it acts up again I will pull the pedal back apart and look closer.
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  9. Default

    Quote Originally Posted by Injected65 View Post
    This weekend I have a bunch of chrome moly welding and a bit of aluminum welding to do. I'll give it a good workout. If it acts up again I will pull the pedal back apart and look closer.
    So what was the deal...is it ok now...any advise for me, as my pedal is doing the same thing as yours was...

  10. Default

    Quote Originally Posted by tnc110 View Post
    So what was the deal...is it ok now...any advise for me, as my pedal is doing the same thing as yours was...
    It went back to working just fine. I welded for 4-5 hours this weekend without one problem. No idea what was up with the pedal but for the time being it is back to working fine.

    Chris
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  11. Default

    Back to not working now. In the middle of a paying job, great timing...........
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  12. #12

    Default

    Quote Originally Posted by Injected65 View Post
    Back to not working now. In the middle of a paying job, great timing...........
    Injected65

    if you need new pedal i will Express you one on Monday
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  13. Default

    Thanks for the offer Oleg. Is there anything that I can/should check to make sure its a foot pedal issue?


    Chris
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  14. #14

    Default

    Chris
    Please get a hold of ray
    He will help you, and I do the rest


    Oleg Gladshteyn
    Oleg@everlastwelders.com
    415 613 664 cell
    650 588 8588 work
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  15. Default

    Will do. I'll try and get a hold of him tomorrow (or Monday by phone if he doesn't see this first).

    Just for and FYI, If you switch the machine to 4T the arc will start but is very low. If you swap to the stock torch switch leads the machine works as it should. I ended up robbing the switch and cable from the stock torch and electrical taped it to my CK torch and got a good bit of the job done tonight.


    Chris
    Everlast Powertig 200DX
    Miller Synchrowave 200
    Miller Dynasty 300 (Work Machine)
    Hobart Handler 210MVP
    HTP Microcut 30

  16. Default

    Quote Originally Posted by Oleg View Post
    Injected65

    if you need new pedal i will Express you one on Monday
    I would like to bring attention to this post. With all the negative stuff floating around about the import welders, has anybody ever seen any other welding company just offer up a free 125.00 foot pedal and pay to ship it? He did this for my friend that has a 250EX. He never talked to my friend, I told him about the issue with his foot control and Oleg shipped me a new foot control for my friend. My friend thanks you!

  17. Default

    You are correct, a big name company would do a full investigation first and send out a forensic to your shop first. I have never experienced the customer service from ANY other company that I have from everlast. There service is amazing.

  18. #18

    Default

    Thank you guys .. we just doing best job we can !
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  19. #19

    Default

    you guys are number one in my book for taking care of us customers

  20. #20

    Default

    Oleg getting a 4x4 cnc plasma table next month let you know how the everlast plasma cutter work got a killer deal on the table kit . Its kit for 1800.00

Similar Threads

  1. Foot Pedal issue. PowerTig 200DX analog
    By Challenger in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 09-14-2014, 02:32 AM
  2. Yet another TIG Foot Pedal issue
    By bswinn in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 01-03-2013, 02:02 AM
  3. pedal issue is fixed!!! now Im really a tigging!!!
    By welderdude in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 07-01-2012, 02:53 AM
  4. 200DX pedal issue - erratic arc
    By Joe from NY in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 01-10-2012, 09:39 PM
  5. Foot pedal issue/tweak.
    By angular in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 03-16-2011, 01:30 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •